Films made from covalent organic frameworks (COFs) are promising materials for a variety of applications, such as membranes for chemical separation, mechanically robust engineering materials, and components of energy storage devices. However, current techniques for synthesizing imine-based COF films use methods that are difficult to scale, produce films of only nanometer-scale thickness, or yield films with modest surface areas and low crystallinity. Here, a facile, scalable process for casting free-standing, imine-based COF films tens of microns in thickness directly from a solution of monomers in trifluoroacetic acid and water is reported for the first time. Highly crystalline films with surface areas (2200–2400 m2/g) approaching the theoretical maximum could be achieved by controlling the initial film formation conditions and by heating the produced films in ethanol with a small amount of residual acid.

KeyWords AITranslate

covalent organic framework 2D polymer films controlled evaporation annealing doctor blade
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01828

Chinese Library Classification Number:

Citation Information:

Films made from covalent organic frameworks (COFs) are promising materials for a variety of applications, such as membranes for chemical separation, mechanically robust engineering materials, and components of energy storage devices. However, current techniques for synthesizing imine-based COF films use methods that are difficult to scale, produce films of only nanometer-scale thickness, or yield films with modest surface areas and low crystallinity. Here, a facile, scalable process for casting free-standing, imine-based COF films tens of microns in thickness directly from a solution of monomers in trifluoroacetic acid and water is reported for the first time. Highly crystalline films with surface areas (2200–2400 m2/g) approaching the theoretical maximum could be achieved by controlling the initial film formation conditions and by heating the produced films in ethanol with a small amount of residual acid.

quote

GB/T 7714-2015 [1] Morgan G. Barnes, David C. McLeod, Robert H. Lambeth. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01828.
MLA [1] Morgan G. Barnes, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01828.
APA [1] Morgan G. Barnes, David C. McLeod, & Robert H. Lambeth. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01828
IEEE [1] Morgan G. Barnes, David C. McLeod, and Robert H. Lambeth, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01828. keywords: {covalent organic framework;2D polymer;films;controlled evaporation;annealing;doctor blade}