Revealing the Crystallization and Thermal-Induced Phase Evolution in Aromatic-Based Quasi-2D Perovskites Using a Robot-Based Platform AITranslate
Abstract AITranslate
Introducing large organic cations to form reduced-dimensional (quasi-2D) perovskites has proven to be effective in stabilizing three-dimensional perovskites. In this study, we synthesized 28 Ruddlesden–Popper-type quasi-2D perovskites using four aromatic-based cations (phenylmethylammonium (PMA), phenethylammonium (PEA), phenylpropylammonium (PPA), and phenylbutanammonium (PBA)) and systematically investigated their optoelectronic and structural properties and thermal stability. A counterintuitive finding that longer-chain PPA-based films exhibited relatively poorer stability compared to films with shorter-chain cations has been found. This instability in PPA-based samples is attributed to significant lattice distortion and a mismatched phase between face-sharing trimers, causing intense configurational strain. On the other hand, PBA-containing films maintained robust structural stability due to distinctive crystallization kinetics and a gradual phase-transformation process (from larger-n to lower-n phases) induced by a stronger steric-hindrance effect. Our study sheds light on the complex impact of aromatic-based cations on optoelectronic properties and stability of perovskites, providing guidelines for the rational compositional design engineering of highly stable perovskite materials.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.3c01508
Chinese Library Classification Number:
Citation Information:
Introducing large organic cations to form reduced-dimensional (quasi-2D) perovskites has proven to be effective in stabilizing three-dimensional perovskites. In this study, we synthesized 28 Ruddlesden–Popper-type quasi-2D perovskites using four aromatic-based cations (phenylmethylammonium (PMA), phenethylammonium (PEA), phenylpropylammonium (PPA), and phenylbutanammonium (PBA)) and systematically investigated their optoelectronic and structural properties and thermal stability. A counterintuitive finding that longer-chain PPA-based films exhibited relatively poorer stability compared to films with shorter-chain cations has been found. This instability in PPA-based samples is attributed to significant lattice distortion and a mismatched phase between face-sharing trimers, causing intense configurational strain. On the other hand, PBA-containing films maintained robust structural stability due to distinctive crystallization kinetics and a gradual phase-transformation process (from larger-n to lower-n phases) induced by a stronger steric-hindrance effect. Our study sheds light on the complex impact of aromatic-based cations on optoelectronic properties and stability of perovskites, providing guidelines for the rational compositional design engineering of highly stable perovskite materials.
quote
| GB/T 7714-2015 | [1] Jiyun Zhang, Jianchang Wu, Yicheng Zhao, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c01508. |
| MLA | [1] Jiyun Zhang, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c01508. |
| APA | [1] Jiyun Zhang, Jianchang Wu, Yicheng Zhao, Yuqin Zou, Anastasia Barabash, Zhenni Wu, Kaicheng Zhang, Can Deng, Jack Elia, Chaohui Li, Juan S. RochaOrtiz, Chao Liu, Abdus Saboor, Ian Marius Peters, Jens A. Hauch, & Christoph J. Brabec. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c01508 |
| IEEE | [1] Jiyun Zhang, Jianchang Wu, Yicheng Zhao, Yuqin Zou, Anastasia Barabash, Zhenni Wu, Kaicheng Zhang, Can Deng, Jack Elia, Chaohui Li, Juan S. RochaOrtiz, Chao Liu, Abdus Saboor, Ian Marius Peters, Jens A. Hauch, and Christoph J. Brabec, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c01508. |