GEMINI — DiagPlot: 2D & 3D ternary phase diagrams AITranslate
Abstract AITranslate
GEMINI is the Gibbs Energy Minimizer of ThermoSuite, a package of chemoinformatics devoted to thermodynamics. In the last years a special effort was made to develop specific procedures to plot 2D & 3D ternary phase diagrams. The Diphasic Domain Approach Method allows us to plot 2D isobarothermic sections in ternary systems with efficiency and robustness. The technique of regular meshing applied to the extremities of the conodes of a set of such isobarothermic ternary sections allows us to go for a trip in the third dimension, giving a deeper understanding of ternary phase diagrams by adding a visual 3D approach.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.calphad.2008.09.007
Chinese Library Classification Number:
Citation Information:
GEMINI is the Gibbs Energy Minimizer of ThermoSuite, a package of chemoinformatics devoted to thermodynamics. In the last years a special effort was made to develop specific procedures to plot 2D & 3D ternary phase diagrams. The Diphasic Domain Approach Method allows us to plot 2D isobarothermic sections in ternary systems with efficiency and robustness. The technique of regular meshing applied to the extremities of the conodes of a set of such isobarothermic ternary sections allows us to go for a trip in the third dimension, giving a deeper understanding of ternary phase diagrams by adding a visual 3D approach.
quote
| GB/T 7714-2015 | [1] Bertrand Cheynet, Catherine Bonnet, Milan Stankov. Calphad, 2009(33). DOI:10.1016/j.calphad.2008.09.007. |
| MLA | [1] Bertrand Cheynet, et al., Calphad, no. 33, 2009, https://doi.org/10.1016/j.calphad.2008.09.007. |
| APA | [1] Bertrand Cheynet, Catherine Bonnet, & Milan Stankov. (2009). Calphad(33). https://doi.org/10.1016/j.calphad.2008.09.007 |