daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Predicting the Volume Phase Transition Temperature of Multi-Responsive Poly(N-isopropylacrylamide)-Based Microgels Using a Cluster-Based Partial Least Squares Modeling Approach AITranslate

McMaster University; McMaster University; McMaster University; McMaster University; McMaster University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Despite the various potential applications of dual pH/temperature-responsive microgels, the multiple (and often interacting) physical and chemical factors that influence the volume phase transition temperature (VPTT) in such microgels make it challenging to directly design a microgel with a particular targeted swelling response. Herein, we address this challenge by designing and implementing a data-driven model that can predict a microgel swelling profile and subsequently VPTT based only on the microgel recipe. A clustering-based adaptation of partial least squares modeling is developed and subsequently applied to a data library of pH 4 (fully protonated) and pH 10 (fully ionized) swelling responses of 32 pH/temperature-responsive poly(N-isopropylacrylamide) microgels functionalized with various carboxylic acid-functionalized comonomers. We demonstrate that the best-performing clustering and data arrangement strategies can predict the VPTT of the microgels within 1.0 °C at pH 4 and 2.4 °C at pH 10, an accuracy similar to the uncertainty estimates from the experimental transition temperature data (0.6 °C at pH 4 and 2.2 °C at pH 10). Such an approach thus paves the way for faster customization of a microgel swelling profile as needed for a target application.

KeyWords AITranslate

pH−temperatureresponsive microgels VPTT latent variable modeling PLS PCA
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01487

Chinese Library Classification Number:

Citation Information:

Despite the various potential applications of dual pH/temperature-responsive microgels, the multiple (and often interacting) physical and chemical factors that influence the volume phase transition temperature (VPTT) in such microgels make it challenging to directly design a microgel with a particular targeted swelling response. Herein, we address this challenge by designing and implementing a data-driven model that can predict a microgel swelling profile and subsequently VPTT based only on the microgel recipe. A clustering-based adaptation of partial least squares modeling is developed and subsequently applied to a data library of pH 4 (fully protonated) and pH 10 (fully ionized) swelling responses of 32 pH/temperature-responsive poly(N-isopropylacrylamide) microgels functionalized with various carboxylic acid-functionalized comonomers. We demonstrate that the best-performing clustering and data arrangement strategies can predict the VPTT of the microgels within 1.0 °C at pH 4 and 2.4 °C at pH 10, an accuracy similar to the uncertainty estimates from the experimental transition temperature data (0.6 °C at pH 4 and 2.2 °C at pH 10). Such an approach thus paves the way for faster customization of a microgel swelling profile as needed for a target application.

quote

GB/T 7714-2015 [1] Seyed Saeid Tayebi, Elizabeth Keane, Nahieli Preciado Rivera, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01487.
MLA [1] Seyed Saeid Tayebi, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01487.
APA [1] Seyed Saeid Tayebi, Elizabeth Keane, Nahieli Preciado Rivera, Todd Hoare, & Prashant Mhaskar. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01487