Free-Standing Sulfur Cathodes Enabled by a Cationic Polymer for Lean Electrolyte Lithium–Sulfur Batteries AITranslate

Fuzhou University; Fuzhou University; Fuzhou University; Fuzhou University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

It is well-known that, under lean electrolyte and high sulfur loading conditions, it is challenging to achieve a high discharge platform, discharge capacity, and cycling stability for lithium–sulfur (Li–S) batteries. Here we report a free-standing sulfur cathode that can efficiently adsorb and electrochemically catalyze polysulfides. A cationic polymer, polyquaternium-10 (P10), is adopted as a new binder that produces viscoelastic fibers during casting, facilitates lithium-ion transportation, and electrostatically regulates polysulfides. The cationic polymer promotes the formation of the free-standing cathode with a desirable web-like microstructure. The Li–S battery constructed by the free-standing cathode with sulfur mass loading of 6 mg cm–2 achieves a high initial areal capacity of 7.09 mAh cm–2 (i.e., 344.5 Wh kg–1 and 471.6 Wh l–1) and stable areal capacity of 4.48 mAh cm–2 (i.e., 217.6 Wh kg–1 and 235.8 Wh l–1) during cycling at a low electrolyte/sulfur ratio of 4 μL mg–1.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.2c02092

Chinese Library Classification Number:

Citation Information:

It is well-known that, under lean electrolyte and high sulfur loading conditions, it is challenging to achieve a high discharge platform, discharge capacity, and cycling stability for lithium–sulfur (Li–S) batteries. Here we report a free-standing sulfur cathode that can efficiently adsorb and electrochemically catalyze polysulfides. A cationic polymer, polyquaternium-10 (P10), is adopted as a new binder that produces viscoelastic fibers during casting, facilitates lithium-ion transportation, and electrostatically regulates polysulfides. The cationic polymer promotes the formation of the free-standing cathode with a desirable web-like microstructure. The Li–S battery constructed by the free-standing cathode with sulfur mass loading of 6 mg cm–2 achieves a high initial areal capacity of 7.09 mAh cm–2 (i.e., 344.5 Wh kg–1 and 471.6 Wh l–1) and stable areal capacity of 4.48 mAh cm–2 (i.e., 217.6 Wh kg–1 and 235.8 Wh l–1) during cycling at a low electrolyte/sulfur ratio of 4 μL mg–1.

quote

GB/T 7714-2015 [1] Hui Chen, Xipin Zhang, Senlin Li, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02092.
MLA [1] Hui Chen, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02092.
APA [1] Hui Chen, Xipin Zhang, Senlin Li, & Yuanhui Zheng. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02092
IEEE [1] Hui Chen, Xipin Zhang, Senlin Li, and Yuanhui Zheng, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02092.