Excellent Wideband Acoustic Absorption of a Multifunctional Composite Fibrous Panel with a Dual-Pore Network from Milled Corrugated Box Wastes AITranslate

Myongji University; Myongji University; Myongji University; Myongji University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A multifunctional composite fibrous sound-absorption panel was acquired via sustainable fabrication from milling corrugated cardboard box wastes to unleash its fibrous property, creating a high-porosity material. Here, a multifunctional composite fibrous panel from the milled fibers of corrugated cardboard boxes reinforced by cross-linked polyvinyl alcohol as a biodegradable binder is generated. It is designed to have a dual-pore structure with a low density of 0.04 g/cm3, which can withstand a load of 5000 times its weight and is effective for the dissipation of sound at a wide range of frequencies. The prepared material demonstrates an excellent average absorption coefficient of 0.83 at wideband frequency, which is about 280–6300 Hz. The outstanding sound absorption performance of the material is primarily ascribed to its dual-pore architecture, the anisotropic pores interconnected by the random pores formed from the collection of cardboard box fibers within the architecture of the porous material, its thickness, and the concentration of corrugated box fibers. Furthermore, the prepared material manifests a unique porous morphological structure, favorable thermal properties, excellent mechanical stability and sustainability, and superhydrophobic properties. The successful fabrication of this riveting material endowed a promising result that may be applicable for various types of applications.

KeyWords AITranslate

multifunctional composite fibrous panel dualpore architecture anisotropic pores random pores dissipation of sound
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01467

Chinese Library Classification Number:

Citation Information:

A multifunctional composite fibrous sound-absorption panel was acquired via sustainable fabrication from milling corrugated cardboard box wastes to unleash its fibrous property, creating a high-porosity material. Here, a multifunctional composite fibrous panel from the milled fibers of corrugated cardboard boxes reinforced by cross-linked polyvinyl alcohol as a biodegradable binder is generated. It is designed to have a dual-pore structure with a low density of 0.04 g/cm3, which can withstand a load of 5000 times its weight and is effective for the dissipation of sound at a wide range of frequencies. The prepared material demonstrates an excellent average absorption coefficient of 0.83 at wideband frequency, which is about 280–6300 Hz. The outstanding sound absorption performance of the material is primarily ascribed to its dual-pore architecture, the anisotropic pores interconnected by the random pores formed from the collection of cardboard box fibers within the architecture of the porous material, its thickness, and the concentration of corrugated box fibers. Furthermore, the prepared material manifests a unique porous morphological structure, favorable thermal properties, excellent mechanical stability and sustainability, and superhydrophobic properties. The successful fabrication of this riveting material endowed a promising result that may be applicable for various types of applications.

quote

GB/T 7714-2015 [1] James Laurence A. Ruello, Arni Gesselle M. Pornea, John Marc C. Puguan, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01467.
MLA [1] James Laurence A. Ruello, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01467.
APA [1] James Laurence A. Ruello, Arni Gesselle M. Pornea, John Marc C. Puguan, & Hern Kim. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01467
IEEE [1] James Laurence A. Ruello, Arni Gesselle M. Pornea, John Marc C. Puguan, and Hern Kim, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01467. keywords: {multifunctional composite fibrous panel;dualpore architecture;anisotropic pores;random pores;dissipation of sound}