Lithium Recovery from Oil and Gas Produced Water: A Need for a Growing Energy Industry AITranslate

Massachusetts Institute of Technology; University of British Columbia; Massachusetts Institute of Technology; Massachusetts Institute of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b00779

Chinese Library Classification Number:

Citation Information:

quote

GB/T 7714-2015 [1] Amit Kumar, Hiroki Fukuda, T. Alan Hatton, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00779.
MLA [1] Amit Kumar, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00779.
APA [1] Amit Kumar, Hiroki Fukuda, T. Alan Hatton, & John H. Lienhard, V. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b00779
IEEE [1] Amit Kumar, Hiroki Fukuda, T. Alan Hatton, and John H. Lienhard, V, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b00779.