Energy and Power Evolution Over the Lifetime of a Battery AITranslate

Pacific Northwest National Laboratory;Pacific Northwest National Laboratory;Pacific Northwest National Laboratory;Pacific Northwest National Laboratory
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00660

Chinese Library Classification Number:

Citation Information:

quote

GB/T 7714-2015 [1] Fredrick Omenya, Matthew Paiss, Xiaolin Li, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00660.
MLA [1] Fredrick Omenya, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00660.
APA [1] Fredrick Omenya, Matthew Paiss, Xiaolin Li, & David Reed. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00660
IEEE [1] Fredrick Omenya, Matthew Paiss, Xiaolin Li, and David Reed, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00660.