daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Iron-Containing Polyhedral Oligomeric Silsesquioxane Assembly Supported on Hexagonal Boron Nitride and Its Effect on Epoxy Resins AITranslate

Beijing Institute of Technology; Beijing Institute of Technology; Beijing Institute of Technology;Shanghai Aerospace Institute of Applied Chemical Engineering; Beijing Institute of Technology; Beijing Institute of Technology; Beijing Institute of Technology; Beijing Institute of Technology; Beijing Institute of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Boron nitride (BN) has great potential to improve the thermal conductivity of polymers, and polyhedral oligomeric silsesquioxane (POSS) revealed the ability to prepare polymers with a low dielectric constant. Combining the two abovementioned materials, an iron-containing polyhedral oligomeric silsesquioxane assembly supported on hexagonal boron nitride (FePOSS@hbno) was prepared via two steps involving hydroxylation and self-aggregation. The morphology of nanohybrid FePOSS@hbno indicated that FePOSS successfully aggregated on the surfaces and edges, which was evidenced by transmission electron microscopy (TEM) and scanning electron microscopy (SEM) images. The nanohybrid was also confirmed by Fourier transform infrared (FTIR) spectroscopy, X-ray diffraction (XRD), and X-ray photoelectron spectroscopy (XPS). The well-characterized FePOSS@hbno was incorporated into epoxy resins, and the thermal conductivity of epoxy composites increased by 104.3% with 20 wt % FePOSS@hbno. The dielectric constant of epoxy composites containing 3.6 wt % FePOSS@hbno clearly decreased in the frequency range of 103–106 Hz. Significantly, 3.6 wt % FePOSS@hbno reduced the peak of the heat release rate by 49.3% and increased the LOI value to 31.2%. Moreover, the condensed and gaseous phases were investigated in detail. The enhanced flame retardancy originated from the nanohybrid structure as well as the elemental merits.

KeyWords AITranslate

POSS boron nitride dielectric constant thermally conductive composites fire resistance
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00641

Chinese Library Classification Number:

Citation Information:

Boron nitride (BN) has great potential to improve the thermal conductivity of polymers, and polyhedral oligomeric silsesquioxane (POSS) revealed the ability to prepare polymers with a low dielectric constant. Combining the two abovementioned materials, an iron-containing polyhedral oligomeric silsesquioxane assembly supported on hexagonal boron nitride (FePOSS@hbno) was prepared via two steps involving hydroxylation and self-aggregation. The morphology of nanohybrid FePOSS@hbno indicated that FePOSS successfully aggregated on the surfaces and edges, which was evidenced by transmission electron microscopy (TEM) and scanning electron microscopy (SEM) images. The nanohybrid was also confirmed by Fourier transform infrared (FTIR) spectroscopy, X-ray diffraction (XRD), and X-ray photoelectron spectroscopy (XPS). The well-characterized FePOSS@hbno was incorporated into epoxy resins, and the thermal conductivity of epoxy composites increased by 104.3% with 20 wt % FePOSS@hbno. The dielectric constant of epoxy composites containing 3.6 wt % FePOSS@hbno clearly decreased in the frequency range of 103–106 Hz. Significantly, 3.6 wt % FePOSS@hbno reduced the peak of the heat release rate by 49.3% and increased the LOI value to 31.2%. Moreover, the condensed and gaseous phases were investigated in detail. The enhanced flame retardancy originated from the nanohybrid structure as well as the elemental merits.

quote

GB/T 7714-2015 [1] Wenyuan Zhang, Zijian Zheng, Jianfeng Huang, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00641.
MLA [1] Wenyuan Zhang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00641.
APA [1] Wenyuan Zhang, Zijian Zheng, Jianfeng Huang, Zhaohong Shen, Boyou Hou, Meiyu Ji, Wenchao Zhang, Zhaolu Qin, & Rongjie Yang. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00641
IEEE [1] Wenyuan Zhang, Zijian Zheng, Jianfeng Huang, Zhaohong Shen, Boyou Hou, Meiyu Ji, Wenchao Zhang, Zhaolu Qin, and Rongjie Yang, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00641. keywords: {POSS;boron nitride;dielectric constant;thermally conductive composites;fire resistance}