Overcoming the Interfacial Challenges of LiFePO4 in Inorganic All-Solid-State Batteries AITranslate

University of California San Diego; University of California San Diego; University of California San Diego; University of California San Diego; University of California San Diego; University of California San Diego; University of California San Diego; University of California San Diego; University of California San Diego; University of California San Diego; University of California San Diego; The University of Chicago
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

All-solid-state batteries (ASSBs) are one of the most promising systems to enable long-lasting and thermally resilient next-generation energy storage. Ideally, these systems should utilize low-cost resources with reduced reliance on critical materials. Pursuing cobalt- and nickel-free chemistries, like LiFePO4 (LFP), is a promising strategy. Morphological features of LFP essential for improved electrochemical performance are highlighted to elucidate the interfacial challenges when implemented in ASSBs, since adoption in inorganic ASSBs has yet to be reported. In this work, the compatibility of LFP with two types of solid-state electrolytes, Li6PS5Cl (LPSCl) and Li2ZrCl6 (LZC), are investigated. The potential existence of oxidative decomposition products is probed using a combination of structural, electrochemical, and spectroscopic analyses. Bulk and interfacial characterization reveal that the sulfide-based electrolyte LPSCl decomposes into insulative products, and electrochemical impedance spectroscopy is used to quantify the resulting impedance growth. However, through utilization of the chloride-based electrolyte LZC, high-rate and stable electrochemical performance is achieved at room temperature.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.2c02138

Chinese Library Classification Number:

Citation Information:

All-solid-state batteries (ASSBs) are one of the most promising systems to enable long-lasting and thermally resilient next-generation energy storage. Ideally, these systems should utilize low-cost resources with reduced reliance on critical materials. Pursuing cobalt- and nickel-free chemistries, like LiFePO4 (LFP), is a promising strategy. Morphological features of LFP essential for improved electrochemical performance are highlighted to elucidate the interfacial challenges when implemented in ASSBs, since adoption in inorganic ASSBs has yet to be reported. In this work, the compatibility of LFP with two types of solid-state electrolytes, Li6PS5Cl (LPSCl) and Li2ZrCl6 (LZC), are investigated. The potential existence of oxidative decomposition products is probed using a combination of structural, electrochemical, and spectroscopic analyses. Bulk and interfacial characterization reveal that the sulfide-based electrolyte LPSCl decomposes into insulative products, and electrochemical impedance spectroscopy is used to quantify the resulting impedance growth. However, through utilization of the chloride-based electrolyte LZC, high-rate and stable electrochemical performance is achieved at room temperature.

quote

GB/T 7714-2015 [1] Ashley Cronk, YuTing Chen, Grayson Deysher, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02138.
MLA [1] Ashley Cronk, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02138.
APA [1] Ashley Cronk, YuTing Chen, Grayson Deysher, SoYeon Ham, Hedi Yang, Phillip Ridley, Baharak Sayahpour, Long Hoang Bao Nguyen, Jin An Sam Oh, Jihyun Jang, Darren H. S. Tan, & Ying Shirley Meng. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02138
IEEE [1] Ashley Cronk, YuTing Chen, Grayson Deysher, SoYeon Ham, Hedi Yang, Phillip Ridley, Baharak Sayahpour, Long Hoang Bao Nguyen, Jin An Sam Oh, Jihyun Jang, Darren H. S. Tan, and Ying Shirley Meng, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02138.