Elastic Aerogel with Tunable Wettability for Self-Cleaning Electronic Skin AITranslate
Abstract AITranslate
Lightweight aerogels with elastic performance and tunable surface properties have made them a good alternative for smart electornic skin. However, the aerogels remain a great barrier for sensing applications because of their severe brittleness and difficult regulation of surface property. Herein, we report a superelastic aerogel originated from a rational designed waterborne poly(siloxane-benzoxazine) by using the ice template method. The three-dimensional (3D) network is constructed via the radical crosslinking and ring-opening polymerization followed by the freeze-drying process. Moreover, it also shows pronounced mechanical performance that can be compressed over 70% and recover without fracture. Beyond that, its surface property could be altered from highly hydrophilic to hydrophobic property (145° water contact angle) by adjusting the crosslinking degree of the aerogel under different curing temperatures. We further demonstrate a pressure sensor by in situ polymerization of the aniline (PANI) on the surface of the aerogel. The multifunctional properties make it an attractive material for self-cleaning electronic skin.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsmaterialslett.0c00464
Chinese Library Classification Number:
Citation Information:
Lightweight aerogels with elastic performance and tunable surface properties have made them a good alternative for smart electornic skin. However, the aerogels remain a great barrier for sensing applications because of their severe brittleness and difficult regulation of surface property. Herein, we report a superelastic aerogel originated from a rational designed waterborne poly(siloxane-benzoxazine) by using the ice template method. The three-dimensional (3D) network is constructed via the radical crosslinking and ring-opening polymerization followed by the freeze-drying process. Moreover, it also shows pronounced mechanical performance that can be compressed over 70% and recover without fracture. Beyond that, its surface property could be altered from highly hydrophilic to hydrophobic property (145° water contact angle) by adjusting the crosslinking degree of the aerogel under different curing temperatures. We further demonstrate a pressure sensor by in situ polymerization of the aniline (PANI) on the surface of the aerogel. The multifunctional properties make it an attractive material for self-cleaning electronic skin.
quote
| GB/T 7714-2015 | [1] Wencan Ma, Zhong Ma, Yifeng Cai, et al. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.0c00464. |
| MLA | [1] Wencan Ma, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.0c00464. |
| APA | [1] Wencan Ma, Zhong Ma, Yifeng Cai, Ruichun Du, Zhicheng Xu, Kefeng Xie, Weizhi Li, Wenbing Hu, Lijia Pan, Qiuhong Zhang, & Xudong Jia. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.0c00464 |
| IEEE | [1] Wencan Ma, Zhong Ma, Yifeng Cai, Ruichun Du, Zhicheng Xu, Kefeng Xie, Weizhi Li, Wenbing Hu, Lijia Pan, Qiuhong Zhang, and Xudong Jia, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.0c00464. |