High-Performance Janus Solar Evaporator for Water Purification with Broad Spectrum Absorption and Ultralow Heat Loss AITranslate

Beihang University; Beihang University; The Australian National University; University of Science & Technology Beijing; Taiyuan University of Technology; Beihang University; Beihang University; Beihang University; Beihang University; Beihang University; Beihang University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Interfacial solar vapor generation offers a promising zero-CO2-consuming energy conversion technology for the production of renewable clean water. The key for boosting solar vapor efficiency relies on the rational design of materials composition and structure at the micro/nanoscale to improve light utilization. Here, we demonstrate a Janus evaporator based on a hydrophilic carbon-black-decorated copper oxide (C@CuO) membrane as the light-absorbing layer and an opposite hydrophobic polymer nanofibers as the thermal insulation layer, which enables efficient energy utilization and vapor generation through a synergistic light absorption and thermal confinement strategy. In addition, the hydrated C@CuO surface reduces vaporization enthalpy that accelerates the efficient evaporation of water. A high evaporation rate of 1.88 kg m–2 h–1 is achieved by the Janus evaporator under 1 sun irradiation. This high photothermal conversion rate and ultralow heat loss synergistic engineering offers a bright future for high-efficiency solar water purification applications.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.2c02567

Chinese Library Classification Number:

Citation Information:

Interfacial solar vapor generation offers a promising zero-CO2-consuming energy conversion technology for the production of renewable clean water. The key for boosting solar vapor efficiency relies on the rational design of materials composition and structure at the micro/nanoscale to improve light utilization. Here, we demonstrate a Janus evaporator based on a hydrophilic carbon-black-decorated copper oxide (C@CuO) membrane as the light-absorbing layer and an opposite hydrophobic polymer nanofibers as the thermal insulation layer, which enables efficient energy utilization and vapor generation through a synergistic light absorption and thermal confinement strategy. In addition, the hydrated C@CuO surface reduces vaporization enthalpy that accelerates the efficient evaporation of water. A high evaporation rate of 1.88 kg m–2 h–1 is achieved by the Janus evaporator under 1 sun irradiation. This high photothermal conversion rate and ultralow heat loss synergistic engineering offers a bright future for high-efficiency solar water purification applications.

quote

GB/T 7714-2015 [1] Lanlan Hou, Nü Wang, LiJuan Yu, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02567.
MLA [1] Lanlan Hou, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02567.
APA [1] Lanlan Hou, Nü Wang, LiJuan Yu, Jingchong Liu, Shaocheng Zhang, Zhimin Cui, Shuai Li, Hui Li, Xiaofei Liu, Lei Jiang, & Yong Zhao. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02567
IEEE [1] Lanlan Hou, Nü Wang, LiJuan Yu, Jingchong Liu, Shaocheng Zhang, Zhimin Cui, Shuai Li, Hui Li, Xiaofei Liu, Lei Jiang, and Yong Zhao, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02567.