Exfoliated 2D Lepidocrocite Titanium Oxide Nanosheets for High Sulfur Content Cathodes with Highly Stable Li–S Battery Performance AITranslate

Ewha Womans University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Despite the high energy densities, lithium–sulfur (Li–S) batteries suffer from insufficient cycle life originating from the shuttling process involving lithium polysulfides (LiPSs). Various approaches have been introduced to resolve the shuttling problem, but they are not usually effective for electrodes with high sulfur contents. Here, we report an exfoliated 2D lepidocrocite titanium oxide nanosheet as a component for sulfur cathodes to suppress polysulfide dissolution markedly. In particular, the Lewis acidity originating from undercoordinated Ti species as well as the large surface area associated with the 2D structure endow 2D lepidocrocite titanium oxide with an efficient interaction with LiPSs. As a result, even with a sulfur content of 80 wt %, the Li–S cell exhibits 1023.5 mAh g–1 at 50 mA g–1 and a capacity retention of 82.3% after 300 cycles measured at 1000 mA g–1. The considerably improved cycling performance provides useful insight for designing sulfur cathodes, that is, the incorporation of acidic 2D metal oxide nanosheets.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.7b01202

Chinese Library Classification Number:

Citation Information:

Despite the high energy densities, lithium–sulfur (Li–S) batteries suffer from insufficient cycle life originating from the shuttling process involving lithium polysulfides (LiPSs). Various approaches have been introduced to resolve the shuttling problem, but they are not usually effective for electrodes with high sulfur contents. Here, we report an exfoliated 2D lepidocrocite titanium oxide nanosheet as a component for sulfur cathodes to suppress polysulfide dissolution markedly. In particular, the Lewis acidity originating from undercoordinated Ti species as well as the large surface area associated with the 2D structure endow 2D lepidocrocite titanium oxide with an efficient interaction with LiPSs. As a result, even with a sulfur content of 80 wt %, the Li–S cell exhibits 1023.5 mAh g–1 at 50 mA g–1 and a capacity retention of 82.3% after 300 cycles measured at 1000 mA g–1. The considerably improved cycling performance provides useful insight for designing sulfur cathodes, that is, the incorporation of acidic 2D metal oxide nanosheets.

quote

GB/T 7714-2015 [1] SeongJu Hwang. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.7b01202.
MLA [1] SeongJu Hwang. ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.7b01202.
APA [1] SeongJu Hwang. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.7b01202
IEEE [1] SeongJu Hwang, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.7b01202.