daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Insights into Stereocomplexation of Poly(lactic acid) Materials: Evolution of Interaction between Enantiomeric Chains and Its Role in Conformational Transformation in Racemic Blends AITranslate

Jiangsu University of Science and Technology; Donghua University; Jiangsu University of Science and Technology; Jiangsu University of Science and Technology; Jiangsu University of Science and Technology; Donghua University; Jiangsu University of Science and Technology;Univ Grenoble Alpes
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Enantiomers alternately packed stereocomplex crystals (SC) compete with homochiral enantiomer-packed homocrystals (HC) during the crystallization of poly(lactic acid) (PLA) racemic blends. However, an intensive understanding of the structural evolution of enantiomeric chains in racemic blends remains challenging because of the narrow time window required for structural evolution. Here, we report the initial conformation evolution and concomitant interaction between the enantiomeric chains in the racemic melt over a wide temperature range using commercial fast-scan chip calorimetry. The results showed that, after cooling the racemic melt at 3,000 K/s, 103 helices always emerged first. The interaction between the enantiomeric chains appeared gradually and triggered the transformation of 103 helices into 31 helices. A comprehensive understanding of the role of the interaction between the enantiomeric chains during the conformation transformation not only provides a physical basis for studying the competition between SC and HC of PLA but also lays a theoretical foundation for the preparation of biodegradable engineering plastics.

KeyWords AITranslate

poly(lactic acid) stereocomplexation interaction between enantiomeric chains conformational transformation Flash DSC Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00781

Chinese Library Classification Number:

Citation Information:

Enantiomers alternately packed stereocomplex crystals (SC) compete with homochiral enantiomer-packed homocrystals (HC) during the crystallization of poly(lactic acid) (PLA) racemic blends. However, an intensive understanding of the structural evolution of enantiomeric chains in racemic blends remains challenging because of the narrow time window required for structural evolution. Here, we report the initial conformation evolution and concomitant interaction between the enantiomeric chains in the racemic melt over a wide temperature range using commercial fast-scan chip calorimetry. The results showed that, after cooling the racemic melt at 3,000 K/s, 103 helices always emerged first. The interaction between the enantiomeric chains appeared gradually and triggered the transformation of 103 helices into 31 helices. A comprehensive understanding of the role of the interaction between the enantiomeric chains during the conformation transformation not only provides a physical basis for studying the competition between SC and HC of PLA but also lays a theoretical foundation for the preparation of biodegradable engineering plastics.

quote

GB/T 7714-2015 [1] Meng Zhang, Xiao Fan, Weijie Guo, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00781.
MLA [1] Meng Zhang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00781.
APA [1] Meng Zhang, Xiao Fan, Weijie Guo, Haijun Zhou, Zhaolei Li, Yu Ma, Chao Yan, & Alain Dufresne. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00781
IEEE [1] Meng Zhang, Xiao Fan, Weijie Guo, Haijun Zhou, Zhaolei Li, Yu Ma, Chao Yan, and Alain Dufresne, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00781. keywords: {poly(lactic acid);stereocomplexation;interaction between enantiomeric chains;conformational transformation;Flash DSC;Show More}