Four-Terminal All-Perovskite Tandem Solar Cells Achieving Power Conversion Efficiencies Exceeding 23% AITranslate
Abstract AITranslate
We report on fabrication of 4-terminal all-perovskite tandem solar cells with power conversion efficiencies exceeding 23% by mechanically stacking semitransparent 1.75 eV wide-bandgap FA0.8Cs0.2Pb(I0.7Br0.3)3 perovskite top cells with 1.25 eV low-bandgap (FASnI3)0.6(MAPbI3)0.4 bottom cells. The top cells use MoOx/ITO transparent electrodes and achieve transmittance up to 70% beyond 700 nm.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.7b01287
Chinese Library Classification Number:
Citation Information:
We report on fabrication of 4-terminal all-perovskite tandem solar cells with power conversion efficiencies exceeding 23% by mechanically stacking semitransparent 1.75 eV wide-bandgap FA0.8Cs0.2Pb(I0.7Br0.3)3 perovskite top cells with 1.25 eV low-bandgap (FASnI3)0.6(MAPbI3)0.4 bottom cells. The top cells use MoOx/ITO transparent electrodes and achieve transmittance up to 70% beyond 700 nm.
quote
| GB/T 7714-2015 | [1] Yanfa Yan. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.7b01287. |
| MLA | [1] Yanfa Yan. ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.7b01287. |
| APA | [1] Yanfa Yan. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.7b01287 |
| IEEE | [1] Yanfa Yan, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.7b01287. |