Multifunctional Conductive Elastomers Based on Tannic Acid and Polymerizable 1-Butyl-3-methylimidazolium Chloride/Acrylic Acid Deep Eutectic Solvent AITranslate
Abstract AITranslate
It is attractive, though challenging, to integrate multiple functions into one conductive elastomer, which can be used in a wide variety of complex scenarios. Here, a series of multifunctional conductive elastomers were fabricated by incorporating various amounts of tannic acid (TA) into the polymerization of 1-butyl-3-methylimidazolium chloride/acrylic acid-type deep eutectic solvent. The obtained conductive elastomers exhibit a combination of desirable properties, including high transparency (an average transmittance of 94.3%), ultrahigh stretchability (1250%), reliable self-healing ability (87.5% healing efficiency for 24 h), favorable conductivity (1.3 × 10–2 mS·cm–1), and excellent temperature tolerance (−20 to 120 °C). Simultaneously, the conductive elastomers showed excellent adhesion to various substrates. Those fabricated conductive elastomer-based sensors could sensitively detect and distinguish various motions with good stability and repeatability from −20 to 120 °C. In addition, we have demonstrated the practical suitability of the fabricated elastomers in constructing flexible electroluminescent devices. The conductive elastomers are believed to show great promise in next-generation wearable electronic devices.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c01804
Chinese Library Classification Number:
Citation Information:
It is attractive, though challenging, to integrate multiple functions into one conductive elastomer, which can be used in a wide variety of complex scenarios. Here, a series of multifunctional conductive elastomers were fabricated by incorporating various amounts of tannic acid (TA) into the polymerization of 1-butyl-3-methylimidazolium chloride/acrylic acid-type deep eutectic solvent. The obtained conductive elastomers exhibit a combination of desirable properties, including high transparency (an average transmittance of 94.3%), ultrahigh stretchability (1250%), reliable self-healing ability (87.5% healing efficiency for 24 h), favorable conductivity (1.3 × 10–2 mS·cm–1), and excellent temperature tolerance (−20 to 120 °C). Simultaneously, the conductive elastomers showed excellent adhesion to various substrates. Those fabricated conductive elastomer-based sensors could sensitively detect and distinguish various motions with good stability and repeatability from −20 to 120 °C. In addition, we have demonstrated the practical suitability of the fabricated elastomers in constructing flexible electroluminescent devices. The conductive elastomers are believed to show great promise in next-generation wearable electronic devices.
quote
| GB/T 7714-2015 | [1] Wei Chen, Wenqing Sun, Jincan Li, et al. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c01804. |
| MLA | [1] Wei Chen, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c01804. |
| APA | [1] Wei Chen, Wenqing Sun, Jincan Li, Yingxuan Qiu, Liyuan Qiu, Jing Ma, Nan Li, & Xingxiang Ji. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c01804 |
| IEEE | [1] Wei Chen, Wenqing Sun, Jincan Li, Yingxuan Qiu, Liyuan Qiu, Jing Ma, Nan Li, and Xingxiang Ji, ACS Applied Polymer Materials, no. 6, 2024, doi: 10.1021/acsapm.3c01804. keywords: {tannic acid;1butyl3methylimidazolium chloride/acrylic acid;polymerizable deep eutectic solvent;conductive elastomers;selfhealing;adhesive;antifreezing} |