daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

A One-Dimensional Organic Lead Chloride Hybrid with Excitation-Dependent Broadband Emissions AITranslate

Fudan University; FAMU-FSU College of Engineering; Oak Ridge National Laboratory; East China Normal University; East China Normal University; Fudan University; Florida State University; Florida State University; Florida State University; Oak Ridge National Laboratory; Florida State University; Fudan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Organic–inorganic metal halide hybrids have emerged as a new class of materials with fascinating optical and electronic properties. The exceptional structure tunability has enabled the development of materials with various dimensionalities at the molecular level, from three-dimensional (3D) to 2D, 1D, and 0D. Here, we report a new 1D lead chloride hybrid, C4N2H14PbCl4, which exhibits unusual inverse excitation-dependent broadband emission from bluish-green to yellow. Density functional theory calculations were performed to better understand the mechanism of this excitation-dependent broadband emission. This 1D hybrid material is found to have two emission centers, corresponding to the self-trapped excitons (STEs) and vacancy-bound excitons. The excitation-dependent emission is due to different populations of these two types of excitons generated at different excitation wavelengths. This work shows the rich chemistry and physics of organic–inorganic metal halide hybrids and paves the way to achieving novel light emitters with excitation-dependent broadband emissions at room temperature.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b00661

Chinese Library Classification Number:

Citation Information:

Organic–inorganic metal halide hybrids have emerged as a new class of materials with fascinating optical and electronic properties. The exceptional structure tunability has enabled the development of materials with various dimensionalities at the molecular level, from three-dimensional (3D) to 2D, 1D, and 0D. Here, we report a new 1D lead chloride hybrid, C4N2H14PbCl4, which exhibits unusual inverse excitation-dependent broadband emission from bluish-green to yellow. Density functional theory calculations were performed to better understand the mechanism of this excitation-dependent broadband emission. This 1D hybrid material is found to have two emission centers, corresponding to the self-trapped excitons (STEs) and vacancy-bound excitons. The excitation-dependent emission is due to different populations of these two types of excitons generated at different excitation wavelengths. This work shows the rich chemistry and physics of organic–inorganic metal halide hybrids and paves the way to achieving novel light emitters with excitation-dependent broadband emissions at room temperature.

quote

GB/T 7714-2015 [1] Guanhong Wu, Chenkun Zhou, Wenmei Ming, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00661.
MLA [1] Guanhong Wu, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00661.
APA [1] Guanhong Wu, Chenkun Zhou, Wenmei Ming, Dan Han, Shiyou Chen, Dong Yang, Tiglet Besara, Jennifer Neu, Theo Siegrist, MaoHua Du, Biwu Ma, & Angang Dong. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00661