daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Single-Atom Electrocatalysts for Lithium Sulfur Batteries: Progress, Opportunities, and Challenges AITranslate

Tianjin University; National University of Singapore; Tianjin University; National University of Singapore; Shenzhen University; Griffith University; Tianjin University; National University of Singapore
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Lithium sulfur (Li–S) battery is considered as one of the most promising energy storage devices, because of its low cost, high energy density, and environmental friendliness. However, the practical applications of Li–S batteries have been hindered by a low utilization efficiency of sulfur arising from complicated chemical conversion of polysulfides and the corrosion of Li metal electrode during charge/discharge processes. Single atom catalysts (SACs) consisting of atomically-dispersed metal sites have been recently exploited as high-performance electrocatalytic materials in various energy storage devices, including Li–S batteries, because of their unique catalytic properties and maximized atom efficiency. In this mini-review, we first describe the major roadblocks and opportunities for the development of commercial Li–S batteries. Following that, we will highlight the specific roles of SAC materials, which are used as cathodes, separators, interlayers, electrolytes, and anodes in Li–S batteries. The detailed catalytic conversion mechanism of polysulfides and nucleation process of Li ions over single-atom active sites are also discussed. Finally, we highlight major challenges to be addressed in this field and provide our perspectives in the rational design and synthesis of superior SACs to accelerate their application in Li–S batteries.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.0c00396

Chinese Library Classification Number:

Citation Information:

Lithium sulfur (Li–S) battery is considered as one of the most promising energy storage devices, because of its low cost, high energy density, and environmental friendliness. However, the practical applications of Li–S batteries have been hindered by a low utilization efficiency of sulfur arising from complicated chemical conversion of polysulfides and the corrosion of Li metal electrode during charge/discharge processes. Single atom catalysts (SACs) consisting of atomically-dispersed metal sites have been recently exploited as high-performance electrocatalytic materials in various energy storage devices, including Li–S batteries, because of their unique catalytic properties and maximized atom efficiency. In this mini-review, we first describe the major roadblocks and opportunities for the development of commercial Li–S batteries. Following that, we will highlight the specific roles of SAC materials, which are used as cathodes, separators, interlayers, electrolytes, and anodes in Li–S batteries. The detailed catalytic conversion mechanism of polysulfides and nucleation process of Li ions over single-atom active sites are also discussed. Finally, we highlight major challenges to be addressed in this field and provide our perspectives in the rational design and synthesis of superior SACs to accelerate their application in Li–S batteries.

quote

GB/T 7714-2015 [1] Feifei Wang, Jing Li, Juan Zhao, et al. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.0c00396.
MLA [1] Feifei Wang, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.0c00396.
APA [1] Feifei Wang, Jing Li, Juan Zhao, Yixiao Yang, Chenliang Su, Yu Lin Zhong, QuanHong Yang, & Jiong Lu. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.0c00396
IEEE [1] Feifei Wang, Jing Li, Juan Zhao, Yixiao Yang, Chenliang Su, Yu Lin Zhong, QuanHong Yang, and Jiong Lu, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.0c00396.