Stable Sn-Based Hybrid Perovskite-Related Structures with Tunable Color Coordinates via Organic Cations in Low-Temperature Synthesis AITranslate
Abstract AITranslate
Organic–inorganic Pb-free layered perovskites are efficient broadband emitters and thus are promising materials for lighting applications. However, their synthetic protocols require a controlled atmosphere, high temperature, and long preparation time. This hinders the potential tunability of their emission through organic cations, as is instead common practice in Pb-based structures. Here, we present a set of Sn–Br layered perovskite-related structures that display different chromaticity coordinates and photoluminescence quantum yield (PLQY) up to 80%, depending on the choice of the organic monocation. We first develop a synthetic protocol that is performed under air and at 4 °C, requiring only a few steps. X-ray and 3D electron diffraction analyses show that the structures exhibit diverse octahedra connectivity (disconnected and face-sharing) and thus optical properties, while preserving the organic–inorganic layer intercalation. These results provide key insight into a previously underexplored strategy to tune the color coordinates of Pb-free layered perovskites through organic cations with complex molecular configurations.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.3c00791
Chinese Library Classification Number:
Citation Information:
Organic–inorganic Pb-free layered perovskites are efficient broadband emitters and thus are promising materials for lighting applications. However, their synthetic protocols require a controlled atmosphere, high temperature, and long preparation time. This hinders the potential tunability of their emission through organic cations, as is instead common practice in Pb-based structures. Here, we present a set of Sn–Br layered perovskite-related structures that display different chromaticity coordinates and photoluminescence quantum yield (PLQY) up to 80%, depending on the choice of the organic monocation. We first develop a synthetic protocol that is performed under air and at 4 °C, requiring only a few steps. X-ray and 3D electron diffraction analyses show that the structures exhibit diverse octahedra connectivity (disconnected and face-sharing) and thus optical properties, while preserving the organic–inorganic layer intercalation. These results provide key insight into a previously underexplored strategy to tune the color coordinates of Pb-free layered perovskites through organic cations with complex molecular configurations.
quote
| GB/T 7714-2015 | [1] Aarya Prabhakaran, Balaji Dhanabalan, Iryna Andrusenko, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00791. |
| MLA | [1] Aarya Prabhakaran, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00791. |
| APA | [1] Aarya Prabhakaran, Balaji Dhanabalan, Iryna Andrusenko, Andrea Pianetti, Simone Lauciello, Mirko Prato, Sergio Marras, Pavlo Solokha, Mauro Gemmi, Sergio Brovelli, Liberato Manna, & Milena P. Arciniegas. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00791 |
| IEEE | [1] Aarya Prabhakaran, Balaji Dhanabalan, Iryna Andrusenko, Andrea Pianetti, Simone Lauciello, Mirko Prato, Sergio Marras, Pavlo Solokha, Mauro Gemmi, Sergio Brovelli, Liberato Manna, and Milena P. Arciniegas, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00791. |