daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Light-Induced Formation of Pb3+ Paramagnetic Species in Lead Halide Perovskites AITranslate

Italy|CNR NANOTEC − Institute of Nanotechnology;Dipartimento di Fisica e Chimica, Università di Palermo; Italy|CNR NANOTEC − Institute of Nanotechnology; Italy|CNR NANOTEC − Institute of Nanotechnology;IC CNR − Istituto di Cristallografia, Via Amendola 122/O;IC CNR − Istituto di Cristallografia, Via Amendola 122/O;IC CNR − Istituto di Cristallografia, Via Amendola 122/O;Dipartimento di Chimica e Chimica Industriale, Università di Pisa;Dipartimento di Chimica e Chimica Industriale, Università di Pisa;Computational Laboratory for Hybrid/Organic Photovoltaics (CLHYO);Dipartimento di Fisica e Chimica, Università di Palermo;Computational Laboratory for Hybrid/Organic Photovoltaics (CLHYO);CNR NANOTEC − Institute of Nanotechnology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Hybrid halide perovskites are soft materials processed at room temperature, revolutionary players in the photovoltaic field. Nowadays, investigation of the nature and role of defects is seen as one of the key challenges toward full comprehension of their behavior and achievement of high device stability under working conditions. We reveal the reversible generation, under illumination, of paramagnetic Pb3+ defects in CH3NH3PbI3, synthesized in ambient conditions, induced by the presence of Pb–O defects in the perovskite structure that may trap photogenerated holes, possibly mediated by the concomitant oxidation and migration of ions. According to the mechanism that we hypothesize, one charge is trapped for each paramagnetic center generated; thus, it does not contribute to the photocurrent, potentially limiting the solar cell performance. Our study, based on combined experimental/theoretical approach, reveals the dynamic evolution of the perovskite characteristics under illumination that needs to be considered when investigating the material physical–chemical properties.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b00944

Chinese Library Classification Number:

Citation Information:

Hybrid halide perovskites are soft materials processed at room temperature, revolutionary players in the photovoltaic field. Nowadays, investigation of the nature and role of defects is seen as one of the key challenges toward full comprehension of their behavior and achievement of high device stability under working conditions. We reveal the reversible generation, under illumination, of paramagnetic Pb3+ defects in CH3NH3PbI3, synthesized in ambient conditions, induced by the presence of Pb–O defects in the perovskite structure that may trap photogenerated holes, possibly mediated by the concomitant oxidation and migration of ions. According to the mechanism that we hypothesize, one charge is trapped for each paramagnetic center generated; thus, it does not contribute to the photocurrent, potentially limiting the solar cell performance. Our study, based on combined experimental/theoretical approach, reveals the dynamic evolution of the perovskite characteristics under illumination that needs to be considered when investigating the material physical–chemical properties.

quote

GB/T 7714-2015 [1] Silvia Colella, Michela Todaro, Sofia Masi, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00944.
MLA [1] Silvia Colella, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00944.
APA [1] Silvia Colella, Michela Todaro, Sofia Masi, Andrea Listorti, Davide Altamura, Rocco Caliandro, Cinzia Giannini, Elisa Carignani, Marco Geppi, Daniele Meggiolaro, Gianpiero Buscarino, Filippo De Angelis, & Aurora Rizzo. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00944
IEEE [1] Silvia Colella, Michela Todaro, Sofia Masi, Andrea Listorti, Davide Altamura, Rocco Caliandro, Cinzia Giannini, Elisa Carignani, Marco Geppi, Daniele Meggiolaro, Gianpiero Buscarino, Filippo De Angelis, and Aurora Rizzo, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00944.