daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Carbon Fiber Reinforced Epoxy Resin Composites with Excellent Recyclable Performance via Dynamic Acylsemicarbazide Moieties AITranslate

Sichuan University; Sichuan University; Sichuan University; Sichuan University; Sichuan University; Sichuan University; Sichuan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Achieving the recycling of the carbon fiber reinforced epoxy resin composite is of great significance toward pursuing a sustainable and circular economy but remains a challenge due to the infusible and insoluble properties of epoxy resin. In this study, the acylsemicarbazide (ASC) moieties are introduced into the network to obtain the dynamic reversible cross-linked thermoset epoxy resin (EPOXY-ASC). An optimized EPOXY-ASC with a tensile stress of 81.27 MPa and an elongation at break of 13.80% exhibits excellent reprocessing performance due to the dynamic reversibility of ASC moieties. The carbon fiber reinforced polymer composites with the EPOXY-ASC resin were successfully prepared with an interlaminar shear strength of 44.86 MPa and can be fully recycled by a solvolysis method without additional agents. The recycled carbon fiber and resin still maintain the original properties well. This study provides a solution to recycle the CFRP composite, which conforms to a circular economy.

KeyWords AITranslate

recycling thermosetting resin carbon fibers laminates mechanical properties
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00658

Chinese Library Classification Number:

Citation Information:

Achieving the recycling of the carbon fiber reinforced epoxy resin composite is of great significance toward pursuing a sustainable and circular economy but remains a challenge due to the infusible and insoluble properties of epoxy resin. In this study, the acylsemicarbazide (ASC) moieties are introduced into the network to obtain the dynamic reversible cross-linked thermoset epoxy resin (EPOXY-ASC). An optimized EPOXY-ASC with a tensile stress of 81.27 MPa and an elongation at break of 13.80% exhibits excellent reprocessing performance due to the dynamic reversibility of ASC moieties. The carbon fiber reinforced polymer composites with the EPOXY-ASC resin were successfully prepared with an interlaminar shear strength of 44.86 MPa and can be fully recycled by a solvolysis method without additional agents. The recycled carbon fiber and resin still maintain the original properties well. This study provides a solution to recycle the CFRP composite, which conforms to a circular economy.

quote

GB/T 7714-2015 [1] Xi Yang, Yindong Wang, Xiaokang Zhang, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00658.
MLA [1] Xi Yang, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00658.
APA [1] Xi Yang, Yindong Wang, Xiaokang Zhang, Zhiwen Jian, Xili Lu, Zhanhua Wang, & Hesheng Xia. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00658