Enhanced Performance and Stability of Poly(carbazole)-Based Anion Exchange Membranes via Synergistic Dual Side Chains for Fuel Cell Applications AITranslate

Shaanxi Normal University; Shaanxi Normal University; Shaanxi Normal University; Shaanxi Normal University; Shaanxi Normal University; Shaanxi Normal University; Shaanxi Normal University; Shaanxi Normal University; Shaanxi Normal University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Anion exchange membranes (AEMs) are crucial components of anion exchange membrane fuel cells (AEMFCs), and the development of highly efficient and stable AEMs is fundamental for advancing the practicality of AEMFCs. In this study, we propose the concept of “combining rigidity and flexibility” to design a series of poly(carbazole)-based AEMs with unique dual side chains. One side chain is a flexible dialkoxy chain, while the other consists of a rigid aromatic structure attached to two flexible alkyl chains. The resulting AEMs exhibit a remarkably high ionic conductivity, ranging from 120.2 to 175.7 mS cm–1 at 80 °C, along with an ion exchange capacity of 1.64–2.19 mequiv g–1. These properties are attributed to significant microphase separation facilitated by the strong interaction between the dual side chains. Furthermore, these AEMs demonstrated excellent alkaline stability. Even after being immersed in NaOH solution for 1080 h, their conductivity remains above 92%. This exceptional stability against hydroxide ions is attributed to the large electrostatic potential of the dialkoxy side chain, as verified by density functional theory calculations. Importantly, when incorporated into a hydrogen–oxygen fuel cell, the AEMs enable the fuel cell to achieve a large power density of 605 mW cm–2 at 70% relative humidity. This remarkable performance underscores their potential application prospects in the field of alkaline fuel cells. As a result, our findings contribute to the ongoing advancement of the AEMFC technology.

KeyWords AITranslate

anion exchange membrane poly(carbazole) ionic conductivity alkaline stability fuel cell
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c02758

Chinese Library Classification Number:

Citation Information:

Anion exchange membranes (AEMs) are crucial components of anion exchange membrane fuel cells (AEMFCs), and the development of highly efficient and stable AEMs is fundamental for advancing the practicality of AEMFCs. In this study, we propose the concept of “combining rigidity and flexibility” to design a series of poly(carbazole)-based AEMs with unique dual side chains. One side chain is a flexible dialkoxy chain, while the other consists of a rigid aromatic structure attached to two flexible alkyl chains. The resulting AEMs exhibit a remarkably high ionic conductivity, ranging from 120.2 to 175.7 mS cm–1 at 80 °C, along with an ion exchange capacity of 1.64–2.19 mequiv g–1. These properties are attributed to significant microphase separation facilitated by the strong interaction between the dual side chains. Furthermore, these AEMs demonstrated excellent alkaline stability. Even after being immersed in NaOH solution for 1080 h, their conductivity remains above 92%. This exceptional stability against hydroxide ions is attributed to the large electrostatic potential of the dialkoxy side chain, as verified by density functional theory calculations. Importantly, when incorporated into a hydrogen–oxygen fuel cell, the AEMs enable the fuel cell to achieve a large power density of 605 mW cm–2 at 70% relative humidity. This remarkable performance underscores their potential application prospects in the field of alkaline fuel cells. As a result, our findings contribute to the ongoing advancement of the AEMFC technology.

quote

GB/T 7714-2015 [1] Ning Xie, Jinchao Han, Haowei Kang, et al. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c02758.
MLA [1] Ning Xie, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c02758.
APA [1] Ning Xie, Jinchao Han, Haowei Kang, Yiting Liu, Qiang Weng, Xingming Ning, Pei Chen, Xinbing Chen, & Zhongwei An. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c02758
IEEE [1] Ning Xie, Jinchao Han, Haowei Kang, Yiting Liu, Qiang Weng, Xingming Ning, Pei Chen, Xinbing Chen, and Zhongwei An, ACS Applied Polymer Materials, no. 6, 2024, doi: 10.1021/acsapm.3c02758. keywords: {anion exchange membrane;poly(carbazole);ionic conductivity;alkaline stability;fuel cell}