Abstract AITranslate

Highlights • Uniaxial strain is key to tuning of material properties, including magnetic phases. • Decoupling effect of type of strain from geometrical effects by forming square lattice. • Compressive strain leads to FM insulator by reduction of Jahn–Teller distortion. • Correlation plays strong role; DFT gives metal, DMFT gives insulator. • Tensile strain give AFM insulator; Flavor of strain is more important than geometry. Recent years have seen tremendous progress in experimental techniques to create uniaxial strain. Motivated by these advances we investigate the effect of uniaxial strain on LaMnO 3 employing ab-initio dynamical mean-field theory, and put it in contrast to biaxial strain that occurs in epitaxial systems. Projecting on the low-energy subspace of Mn 3 d states, and solving multi-impurity problems, our approach emphasizes on local dynamic correlations at Mn sites. At ambient pressures, LaMnO 3 crystallizes in an orthorhombic unit cell, with in-plane lattice constants a < b , and shows an A-type antiferromagnetic ground state. If we apply uniaxial compressive strain such that the in-plane lattice becomes square with lattice constant a , we find a ferromagnetic insulating state. This is in sharp contrast to DFT results using various functionals like PBE, PBE+ U , and hybrid functionals like HSE, which all predict a half-metallic ferromagnetic behavior. Interestingly, applying uniaxial tensile strain, such that the in-plane lattice becomes square with the longer lattice constant b , an antiferromagnetic insulating state is observed. We trace back these results to the reduction in Jahn–Teller distortion in the case of compressive strain, favoring a ferromagnetic state. This reduction is absent in the tensile case, and the antiferromagnetic state therefore survives. Our study shows that it is the flavor of the strain (compressive or tensile) which is decisive for the magnitude of Jahn–Teller distortions and, hence, the magnetic state. Graphical abstract Download : Download high-res image (226KB) Download : Download full-size image

KeyWords AITranslate

DMFT Manganites Uniaxial strain Dynamic correlations Magnetic phase transitions
No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2024.112890

Chinese Library Classification Number:

Citation Information:

Highlights • Uniaxial strain is key to tuning of material properties, including magnetic phases. • Decoupling effect of type of strain from geometrical effects by forming square lattice. • Compressive strain leads to FM insulator by reduction of Jahn–Teller distortion. • Correlation plays strong role; DFT gives metal, DMFT gives insulator. • Tensile strain give AFM insulator; Flavor of strain is more important than geometry. Recent years have seen tremendous progress in experimental techniques to create uniaxial strain. Motivated by these advances we investigate the effect of uniaxial strain on LaMnO 3 employing ab-initio dynamical mean-field theory, and put it in contrast to biaxial strain that occurs in epitaxial systems. Projecting on the low-energy subspace of Mn 3 d states, and solving multi-impurity problems, our approach emphasizes on local dynamic correlations at Mn sites. At ambient pressures, LaMnO 3 crystallizes in an orthorhombic unit cell, with in-plane lattice constants a < b , and shows an A-type antiferromagnetic ground state. If we apply uniaxial compressive strain such that the in-plane lattice becomes square with lattice constant a , we find a ferromagnetic insulating state. This is in sharp contrast to DFT results using various functionals like PBE, PBE+ U , and hybrid functionals like HSE, which all predict a half-metallic ferromagnetic behavior. Interestingly, applying uniaxial tensile strain, such that the in-plane lattice becomes square with the longer lattice constant b , an antiferromagnetic insulating state is observed. We trace back these results to the reduction in Jahn–Teller distortion in the case of compressive strain, favoring a ferromagnetic state. This reduction is absent in the tensile case, and the antiferromagnetic state therefore survives. Our study shows that it is the flavor of the strain (compressive or tensile) which is decisive for the magnitude of Jahn–Teller distortions and, hence, the magnetic state. Graphical abstract Download : Download high-res image (226KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Florian P. Lindner, Markus Aichhorn, Hrishit Banerjee. Computational Materials Science, 2024(237). DOI:10.1016/j.commatsci.2024.112890.
MLA [1] Florian P. Lindner, et al., Computational Materials Science, no. 237, 2024, https://doi.org/10.1016/j.commatsci.2024.112890.
APA [1] Florian P. Lindner, Markus Aichhorn, & Hrishit Banerjee. (2024). Computational Materials Science(237). https://doi.org/10.1016/j.commatsci.2024.112890
IEEE [1] Florian P. Lindner, Markus Aichhorn, and Hrishit Banerjee, Computational Materials Science, no. 237, 2024, doi: 10.1016/j.commatsci.2024.112890. keywords: {DMFT;Manganites;Uniaxial strain;Dynamic correlations;Magnetic phase transitions}