A Hyper-Cross-Linked Aerogel with Rigid Conjugated Polymers as Building Blocks for Efficient Iodine Capture AITranslate
Abstract AITranslate
Porous organic polymers are typically synthesized through coupling reactions between multifunctional monomers. While rich-pore structures can be generated with long building blocks, the synthesis of molecules with functional groups of large spatial separation is challenging. Herein, we report a strategy using conjugated polymers as the long and rigid building blocks. A hyper-cross-linked polymer was synthesized through a click reaction between the internal alkyne units in conjugated polymers and a triazido-compound to give an organogel with a hierarchical porous structure. Benefitting from the rich π electrons and aromatic structures of the hyper-cross-linked polymer networks, the organic aerogel derived from the rigid conjugated polymer-based organogel exhibits a fast adsorption rate and high adsorption capacity for iodine in both aqueous and gas phases. The capture efficiency of the aerogel for iodine in saturated iodine aqueous solution exceeded 80% within 5 min, and the adsorption equilibrium capacity of 3.28 g g–1 for iodine vapor was achieved within 60 min. In addition, the iodine-loaded aerogel has excellent retention in air and can be recycled after thermal release.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c00411
Chinese Library Classification Number:
Citation Information:
Porous organic polymers are typically synthesized through coupling reactions between multifunctional monomers. While rich-pore structures can be generated with long building blocks, the synthesis of molecules with functional groups of large spatial separation is challenging. Herein, we report a strategy using conjugated polymers as the long and rigid building blocks. A hyper-cross-linked polymer was synthesized through a click reaction between the internal alkyne units in conjugated polymers and a triazido-compound to give an organogel with a hierarchical porous structure. Benefitting from the rich π electrons and aromatic structures of the hyper-cross-linked polymer networks, the organic aerogel derived from the rigid conjugated polymer-based organogel exhibits a fast adsorption rate and high adsorption capacity for iodine in both aqueous and gas phases. The capture efficiency of the aerogel for iodine in saturated iodine aqueous solution exceeded 80% within 5 min, and the adsorption equilibrium capacity of 3.28 g g–1 for iodine vapor was achieved within 60 min. In addition, the iodine-loaded aerogel has excellent retention in air and can be recycled after thermal release.
quote
| GB/T 7714-2015 | [1] Zhikun Shang, Fangxu Pu, Xuezheng Zhang, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00411. |
| MLA | [1] Zhikun Shang, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00411. |
| APA | [1] Zhikun Shang, Fangxu Pu, Xuezheng Zhang, Huixian Jin, Shiyong Chen, Yun Ding, & Aiguo Hu. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00411 |
| IEEE | [1] Zhikun Shang, Fangxu Pu, Xuezheng Zhang, Huixian Jin, Shiyong Chen, Yun Ding, and Aiguo Hu, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00411. keywords: {hypercrosslinked aerogel;polymers building blocks;macropores;iodine capture;conjugated polymer} |