Batch-Reproducible and Thickness-Insensitive Mesopolymer Zwitterion Interlayers for Organic Solar Cells AITranslate

Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Peking University; Peking University; University of Massachusetts Amherst; Beijing University of Chemical Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Zwitterionic polymers or small molecules are a class of widely used interlayer materials in organic solar cells (OSCs). It is challenging to develop such materials that combine good film-forming property, high batch-to-batch reproducibility, and broad thickness processing window in device applications. Herein, we designed and synthesized two self-doped conjugated mesopolymer zwitterions (CMZs), namely, MT2PDIMz and MT2PDINz (PDI = perylene-diimide, M = mesopolymer, T2 = dithiophene, Mz = imidazolium zwitterion, Nz = ammonium zwitterion). Both show good processability and effectively reduce the work function of metal electrodes. The substitution of imidazolium cations with ammonium cations on the side-chains can further modulate the solution assembly and self-doping effect of CMZs, enabling improved interfacial compatibility with active layers and higher electron mobility in MT2PDIMz. The versatility of CMZs interlayers for OSCs is confirmed with several binary and ternary active layers, affording efficiencies up to 19.01%. Notably, over 98% of the optimal efficiency is maintained as the thickness of the interlayers increases to 40 nm with good reproducibility.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00584

Chinese Library Classification Number:

Citation Information:

Zwitterionic polymers or small molecules are a class of widely used interlayer materials in organic solar cells (OSCs). It is challenging to develop such materials that combine good film-forming property, high batch-to-batch reproducibility, and broad thickness processing window in device applications. Herein, we designed and synthesized two self-doped conjugated mesopolymer zwitterions (CMZs), namely, MT2PDIMz and MT2PDINz (PDI = perylene-diimide, M = mesopolymer, T2 = dithiophene, Mz = imidazolium zwitterion, Nz = ammonium zwitterion). Both show good processability and effectively reduce the work function of metal electrodes. The substitution of imidazolium cations with ammonium cations on the side-chains can further modulate the solution assembly and self-doping effect of CMZs, enabling improved interfacial compatibility with active layers and higher electron mobility in MT2PDIMz. The versatility of CMZs interlayers for OSCs is confirmed with several binary and ternary active layers, affording efficiencies up to 19.01%. Notably, over 98% of the optimal efficiency is maintained as the thickness of the interlayers increases to 40 nm with good reproducibility.

quote

GB/T 7714-2015 [1] Chenghao Zhu, Jing Tian, Wenxu Liu, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00584.
MLA [1] Chenghao Zhu, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00584.
APA [1] Chenghao Zhu, Jing Tian, Wenxu Liu, Yuxin Duan, Yanan Song, Zuhao You, Xu Wang, Nan Li, Xiaowei Zhan, Thomas P. Russell, & Yao Liu. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00584
IEEE [1] Chenghao Zhu, Jing Tian, Wenxu Liu, Yuxin Duan, Yanan Song, Zuhao You, Xu Wang, Nan Li, Xiaowei Zhan, Thomas P. Russell, and Yao Liu, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00584.