Ultrastretchable and Compact Zn-MnO2 Rechargeable Battery AITranslate
Abstract AITranslate
The rise of stretchable electronics calls for deformable forms of rechargeable batteries as compatible power sources. The crumpled electrode design is a promising avenue for stretchable batteries by providing sufficient internal space to accommodate tensile deformations. Current electrodes typically have rough surfaces with visible corrugations, which present practical challenges in assembling compact cells for wearable systems. In this study, we report the design and preparation of ultrastretchable electrodes with microwrinkled surface textures. Crumpled electrodes are created in a transfer-printing process based on active materials deposited on metal film current collectors. A polymer membrane is introduced as a key mechanical support to effectively enhance the durability of these electrodes against large and repetitive tensile strains. A stretchable pouch cell of Zn-MnO2 rechargeable battery is constructed with a total thickness of ∼1 mm. The battery cell demonstrates a high specific capacity of 211 mAh g–1, stable charge–discharge cycling performances, and ultrahigh deformability of up to 525% strain. The compact design allows the battery to achieve conformal attachment to the skin and versatile integration with various deformable systems. The present work offers a generic approach to creating highly stretchable batteries with microwrinkled electrodes.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsmaterialslett.3c00058
Chinese Library Classification Number:
Citation Information:
The rise of stretchable electronics calls for deformable forms of rechargeable batteries as compatible power sources. The crumpled electrode design is a promising avenue for stretchable batteries by providing sufficient internal space to accommodate tensile deformations. Current electrodes typically have rough surfaces with visible corrugations, which present practical challenges in assembling compact cells for wearable systems. In this study, we report the design and preparation of ultrastretchable electrodes with microwrinkled surface textures. Crumpled electrodes are created in a transfer-printing process based on active materials deposited on metal film current collectors. A polymer membrane is introduced as a key mechanical support to effectively enhance the durability of these electrodes against large and repetitive tensile strains. A stretchable pouch cell of Zn-MnO2 rechargeable battery is constructed with a total thickness of ∼1 mm. The battery cell demonstrates a high specific capacity of 211 mAh g–1, stable charge–discharge cycling performances, and ultrahigh deformability of up to 525% strain. The compact design allows the battery to achieve conformal attachment to the skin and versatile integration with various deformable systems. The present work offers a generic approach to creating highly stretchable batteries with microwrinkled electrodes.
quote
| GB/T 7714-2015 | [1] Kang Ji, Sisi Li, Yong Lin, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c00058. |
| MLA | [1] Kang Ji, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c00058. |
| APA | [1] Kang Ji, Sisi Li, Yong Lin, Jiaxue Zhang, Menglu Wang, Chong Bai, & Desheng Kong. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c00058 |
| IEEE | [1] Kang Ji, Sisi Li, Yong Lin, Jiaxue Zhang, Menglu Wang, Chong Bai, and Desheng Kong, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c00058. |