Self-Healing Hydrogels: From Synthesis to Multiple Applications AITranslate
Abstract AITranslate
Due to the good reliability and long-term stability, self-healing hydrogels have emerged as promising soft materials for tissue engineering, smart wearable sensors, bioelectronics, and energy storage devices. The self-healing mechanism depends on reversible chemical or physical cross-linking interactions. Self-healing hydrogels with fascinating features (including mechanical performances, biocompatibility, conductivity, antibacterial ability, responsiveness, etc.) are being designed and developed according to the practical application requirements. In this review, the recent progress on self-healing hydrogels in their synthesis strategies and multiple applications is summarized. Their synthesis strategies involve reversible chemical or physical cross-linking processes or a combination of the two. Their recent applications include flexible strain sensors, supercapacitors, actuators, adhesives, wound healing, drug delivery, tumor treatment, 3D printing, etc. Finally, the current challenges, future development, and opportunities for self-healing hydrogels are discussed.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsmaterialslett.3c00320
Chinese Library Classification Number:
Citation Information:
Due to the good reliability and long-term stability, self-healing hydrogels have emerged as promising soft materials for tissue engineering, smart wearable sensors, bioelectronics, and energy storage devices. The self-healing mechanism depends on reversible chemical or physical cross-linking interactions. Self-healing hydrogels with fascinating features (including mechanical performances, biocompatibility, conductivity, antibacterial ability, responsiveness, etc.) are being designed and developed according to the practical application requirements. In this review, the recent progress on self-healing hydrogels in their synthesis strategies and multiple applications is summarized. Their synthesis strategies involve reversible chemical or physical cross-linking processes or a combination of the two. Their recent applications include flexible strain sensors, supercapacitors, actuators, adhesives, wound healing, drug delivery, tumor treatment, 3D printing, etc. Finally, the current challenges, future development, and opportunities for self-healing hydrogels are discussed.
quote
| GB/T 7714-2015 | [1] Hongyan Yin, Fangfei Liu, Tursun Abdiryim, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c00320. |
| MLA | [1] Hongyan Yin, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c00320. |
| APA | [1] Hongyan Yin, Fangfei Liu, Tursun Abdiryim, & Xiong Liu. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c00320 |
| IEEE | [1] Hongyan Yin, Fangfei Liu, Tursun Abdiryim, and Xiong Liu, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c00320. |