Solvent-Free and Recyclable Polyether/Polyphenol Supramolecular Adhesives with Robust, Water- and Low-Temperature-Resistant Properties AITranslate

Nanchang University; University of Chinese Academy of Sciences; Institute of Process Engineering; Institute of Process Engineering; Institute of Process Engineering; University of Chinese Academy of Sciences
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Adhesives are widely used in everyday life; however, traditional polymer adhesives pose unavoidable hazards to the environment and living organisms due to their extensive use of toxic organic solvents, heavy reliance on fossil resources as synthetic raw materials, and lack of recyclability. Furthermore, they are incapable of maintaining a stable adhesion performance in harsh conditions. In this work, we present a facile yet powerful noncovalent bonding strategy for successfully constructing poly(glycidol-co-1,2-butylene oxide)/tannic acid supramolecular adhesives (PG-co-PBO/TA SAs) through hydrogen-bonding interactions between hyperbranched PG-co-PBO and natural TA. The SAs demonstrate an adhesion strength of 2.15 MPa at ambient temperature and maintain an adhesion strength of 1.53 MPa even at −196 °C. Moreover, it can be easily recycled through thermal treatment and retains stable adhesion strength even after undergoing multiple recycling cycles. The investigation of the structure–property relationship of SAs and molecular dynamics simulations has clarified that short alkyl chains of PG-co-PBO effectively protect the hydrogen-bonding networks from damage by repelling water at the adhesive interface. Consequently, SAs even maintain robust and long-lasting adhesion strength in acidic, alkaline, and seawater solutions. Importantly, unlike conventional adhesives, SAs do not employ organic solvents throughout the synthesis, bonding, and recycling processes. By designing functionalized polymers and utilizing polyphenolic compounds, this work provides a green and feasible strategy for the development of next-generation powerful supramolecular adhesives.

KeyWords AITranslate

green supramolecular adhesives solventfree recycling lowtemperature resistance water resistance high adhesion strength
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c02376

Chinese Library Classification Number:

Citation Information:

Adhesives are widely used in everyday life; however, traditional polymer adhesives pose unavoidable hazards to the environment and living organisms due to their extensive use of toxic organic solvents, heavy reliance on fossil resources as synthetic raw materials, and lack of recyclability. Furthermore, they are incapable of maintaining a stable adhesion performance in harsh conditions. In this work, we present a facile yet powerful noncovalent bonding strategy for successfully constructing poly(glycidol-co-1,2-butylene oxide)/tannic acid supramolecular adhesives (PG-co-PBO/TA SAs) through hydrogen-bonding interactions between hyperbranched PG-co-PBO and natural TA. The SAs demonstrate an adhesion strength of 2.15 MPa at ambient temperature and maintain an adhesion strength of 1.53 MPa even at −196 °C. Moreover, it can be easily recycled through thermal treatment and retains stable adhesion strength even after undergoing multiple recycling cycles. The investigation of the structure–property relationship of SAs and molecular dynamics simulations has clarified that short alkyl chains of PG-co-PBO effectively protect the hydrogen-bonding networks from damage by repelling water at the adhesive interface. Consequently, SAs even maintain robust and long-lasting adhesion strength in acidic, alkaline, and seawater solutions. Importantly, unlike conventional adhesives, SAs do not employ organic solvents throughout the synthesis, bonding, and recycling processes. By designing functionalized polymers and utilizing polyphenolic compounds, this work provides a green and feasible strategy for the development of next-generation powerful supramolecular adhesives.

quote

GB/T 7714-2015 [1] Xianqiang Zeng, Liguo Wang, Yan Cao, et al. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c02376.
MLA [1] Xianqiang Zeng, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c02376.
APA [1] Xianqiang Zeng, Liguo Wang, Yan Cao, Peng He, Xiaoxuan Wang, & Huiquan Li. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c02376
IEEE [1] Xianqiang Zeng, Liguo Wang, Yan Cao, Peng He, Xiaoxuan Wang, and Huiquan Li, ACS Applied Polymer Materials, no. 6, 2024, doi: 10.1021/acsapm.3c02376. keywords: {green supramolecular adhesives;solventfree recycling;lowtemperature resistance;water resistance;high adhesion strength}