Ordered Lithium-Ion Conductive Interphase with Gradient Desolvation Effects for Fast-Charging Lithium Metal Batteries AITranslate

Shandong University; Shandong University; Shandong University; Shandong University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Efficient desolvation and fast lithium ion (Li+) transport are key factors for fast-charging Li metal batteries (LMBs). Here, we report a self-assembled interphase (SAI) with ordered Li+ transport pathways to enable high Li+ conductivity and fast Li+ desolvation for fast-charging LMBs. A self-assembled structure originating from the intermolecular π–π stacking endows SAI with ordered Li+ transport pathways. The regular molecular stacking and a gradient distribution of functional groups of SAI contribute to a spatially confined gradient desolvation of Li+. Thereby, a stable Li metal anode (LMA) with durable solid-electrolyte interphase, accelerated Li+ transfer, and homogeneous Li plating/stripping is achieved at high rates. A full-cell battery of SAI protected LMA|LiNi0.8Co0.1Mn0.1O2 delivers a high capacity of 147 mAh g–1 with an improved capacity retention for 500 cycles at 3 C (1 C = 210 mA g–1), and the full cell can deliver over 71% of its capacity in 12 min.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00917

Chinese Library Classification Number:

Citation Information:

Efficient desolvation and fast lithium ion (Li+) transport are key factors for fast-charging Li metal batteries (LMBs). Here, we report a self-assembled interphase (SAI) with ordered Li+ transport pathways to enable high Li+ conductivity and fast Li+ desolvation for fast-charging LMBs. A self-assembled structure originating from the intermolecular π–π stacking endows SAI with ordered Li+ transport pathways. The regular molecular stacking and a gradient distribution of functional groups of SAI contribute to a spatially confined gradient desolvation of Li+. Thereby, a stable Li metal anode (LMA) with durable solid-electrolyte interphase, accelerated Li+ transfer, and homogeneous Li plating/stripping is achieved at high rates. A full-cell battery of SAI protected LMA|LiNi0.8Co0.1Mn0.1O2 delivers a high capacity of 147 mAh g–1 with an improved capacity retention for 500 cycles at 3 C (1 C = 210 mA g–1), and the full cell can deliver over 71% of its capacity in 12 min.

quote

GB/T 7714-2015 [1] Congying Song, Jingteng Zhao, Shaobo Ma, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00917.
MLA [1] Congying Song, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00917.
APA [1] Congying Song, Jingteng Zhao, Shaobo Ma, & Guoxing Li. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00917
IEEE [1] Congying Song, Jingteng Zhao, Shaobo Ma, and Guoxing Li, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00917.