daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Polyethylene-Grafted Sheet-like Silsesquioxane Nanocomposites with Unprecedented Adhesion to Polar Substrates AITranslate

Indian Institute of Technology Bombay; CSIR-National Chemical Laboratory; Indian Institute of Technology; CSIR-National Chemical Laboratory; Indian Institute of Technology Bombay
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Polyethylene is a highly apolar polymer with very poor adhesion to most substrates, necessitating the use of tie layers. Therefore, the synthesis of functional polyethylene is a long-standing challenge in catalytic ethylene polymerization. Here, we report the preparation of a nanocomposite comprising polyethylene covalently grafted onto sheet-like silsesquioxanes, with unprecedented adhesion to metal and glass. A norbornene-grafted, layered Mg-silsesquioxane is treated with Grubbs second-generation catalyst (G-II), and the identity of covalently tethered G-II is unambiguously ascertained. Covalently tethered G-II catalyzes the ring opening metathesis polymerization of cyclooctene to poly(cyclooctene). The resulting poly(cyclooctene) is catalytically hydrogenated to yield polyethylene. This polyethylene nanocomposite exhibited a bonding strength of the order of 100 MPa on stainless steel and aluminum, 10-fold higher than reported for engineered polyethylene copolymers. The nanocomposite exhibits an increase in the polar component of surface energy, yet remains compatible and cocrystallizes with a polyethylene matrix.

KeyWords AITranslate

polyethylene clay silsesquioxane nanocomposite adhesion
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00649

Chinese Library Classification Number:

Citation Information:

Polyethylene is a highly apolar polymer with very poor adhesion to most substrates, necessitating the use of tie layers. Therefore, the synthesis of functional polyethylene is a long-standing challenge in catalytic ethylene polymerization. Here, we report the preparation of a nanocomposite comprising polyethylene covalently grafted onto sheet-like silsesquioxanes, with unprecedented adhesion to metal and glass. A norbornene-grafted, layered Mg-silsesquioxane is treated with Grubbs second-generation catalyst (G-II), and the identity of covalently tethered G-II is unambiguously ascertained. Covalently tethered G-II catalyzes the ring opening metathesis polymerization of cyclooctene to poly(cyclooctene). The resulting poly(cyclooctene) is catalytically hydrogenated to yield polyethylene. This polyethylene nanocomposite exhibited a bonding strength of the order of 100 MPa on stainless steel and aluminum, 10-fold higher than reported for engineered polyethylene copolymers. The nanocomposite exhibits an increase in the polar component of surface energy, yet remains compatible and cocrystallizes with a polyethylene matrix.

quote

GB/T 7714-2015 [1] Vivek Sharma, Uday Paulbudhe, Nirmalya Bachhar, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00649.
MLA [1] Vivek Sharma, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00649.
APA [1] Vivek Sharma, Uday Paulbudhe, Nirmalya Bachhar, Samir H. Chikkali, & Guruswamy Kumaraswamy. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00649
IEEE [1] Vivek Sharma, Uday Paulbudhe, Nirmalya Bachhar, Samir H. Chikkali, and Guruswamy Kumaraswamy, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00649. keywords: {polyethylene;clay;silsesquioxane;nanocomposite;adhesion}