N,N′,N″-tripivaloyl-1,3,5-triaminobenzene (XT386) has been proven to be a highly efficient nucleating agent (NA) for polypropylene (PP), though it remains relatively expensive, which hinders its broader adoption. Herein, a methyl addition to benzene and a side-chain engineering strategy on XT386 led to the discovery of N,N′,N″-triacetyl-1,3,5-triaminotoluene (1a) as a very efficient NA for PP. It could raise the crystallization temperature (Tc) of iPP by 10.0 °C at a content not exceeding 1 wt %, reduce haze by 12.3, and increase tensile strength by 4.9 MPa. Refinement of PXRD data revealed that 1a has a c-axis size (∼6.5 Å) similar to PP, which has the ability to form epitaxial matching. Considering that 1a could be made from retired 2,4,6-trinitrotoluene (TNT) by a simple and green procedure of hydrogenation followed by N,N′,N″-triacylation, it will be a very promising NA for PP with good cost performance in the near future.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c02342
Chinese Library Classification Number:
Citation Information:
N,N′,N″-tripivaloyl-1,3,5-triaminobenzene (XT386) has been proven to be a highly efficient nucleating agent (NA) for polypropylene (PP), though it remains relatively expensive, which hinders its broader adoption. Herein, a methyl addition to benzene and a side-chain engineering strategy on XT386 led to the discovery of N,N′,N″-triacetyl-1,3,5-triaminotoluene (1a) as a very efficient NA for PP. It could raise the crystallization temperature (Tc) of iPP by 10.0 °C at a content not exceeding 1 wt %, reduce haze by 12.3, and increase tensile strength by 4.9 MPa. Refinement of PXRD data revealed that 1a has a c-axis size (∼6.5 Å) similar to PP, which has the ability to form epitaxial matching. Considering that 1a could be made from retired 2,4,6-trinitrotoluene (TNT) by a simple and green procedure of hydrogenation followed by N,N′,N″-triacylation, it will be a very promising NA for PP with good cost performance in the near future.
quote
| GB/T 7714-2015 | [1] BoHan Liu, ZhiHui Lin, Xin Qian, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c02342. |
| MLA | [1] BoHan Liu, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c02342. |
| APA | [1] BoHan Liu, ZhiHui Lin, Xin Qian, Ming Tang, BiHong Chi, XinFeng Yang, Jiao Wei, & MuHua Huang. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c02342 |
| IEEE | [1] BoHan Liu, ZhiHui Lin, Xin Qian, Ming Tang, BiHong Chi, XinFeng Yang, Jiao Wei, and MuHua Huang, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c02342. keywords: {polypropylene (PP);nucleating agent (NA);clarifier;N;N′;N″triacyl2;4;6triaminotoluene;circular economy} |