daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

An assessment of finite element analysis to predict the elastic modulus and Poisson’s ratio of singlewall carbon nanotubes AITranslate

Centro de Investigación Científica de Yucatán, Calle 43 No. 130; Universidad Autónoma de Yucatán;Centro de Investigación Científica de Yucatán, Calle 43 No. 130
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Highlights • The elastic modulus and Poisson’s ratio of SWCNTs were obtained by DFT and FEA. • A good correlation between the DFT and FEA was obtained. • The limitations of FEA to predict such elastic properties were assessed. • A set of bond stiffness constants for SWCNTs was calibrated for its use in FEA. Molecular mechanics implemented in finite element codes is becoming a popular method to predict elastic properties of carbon nanotubes. However, the limits of application of this approach have not yet been systematically assessed. Therefore, this work investigates the accuracy and range of application of finite element analysis (FEA) to predict the elastic modulus and Poisson’s ratio of singlewall carbon nanotubes (SWCNTs), by comparing predictions of FEA to ab initio computations based on density functional theory (DFT). FEA predicts an elastic modulus which agrees well with DFT for SWCNTs with diameters larger than 0.8 nm. FEA underpredicts the Poisson’s ratio with respect to DFT, unless the FEA bond force constants previously computed for benzene are adjusted. The use of adequate values of bond force constants and the equilibrium configuration of atomic coordinates predicted by DFT as the input geometry for FEA improves its predictions. The significance of the numerical values chosen for the bond force constants in FEA is also discussed.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2013.10.003

Chinese Library Classification Number:

Citation Information:

Highlights • The elastic modulus and Poisson’s ratio of SWCNTs were obtained by DFT and FEA. • A good correlation between the DFT and FEA was obtained. • The limitations of FEA to predict such elastic properties were assessed. • A set of bond stiffness constants for SWCNTs was calibrated for its use in FEA. Molecular mechanics implemented in finite element codes is becoming a popular method to predict elastic properties of carbon nanotubes. However, the limits of application of this approach have not yet been systematically assessed. Therefore, this work investigates the accuracy and range of application of finite element analysis (FEA) to predict the elastic modulus and Poisson’s ratio of singlewall carbon nanotubes (SWCNTs), by comparing predictions of FEA to ab initio computations based on density functional theory (DFT). FEA predicts an elastic modulus which agrees well with DFT for SWCNTs with diameters larger than 0.8 nm. FEA underpredicts the Poisson’s ratio with respect to DFT, unless the FEA bond force constants previously computed for benzene are adjusted. The use of adequate values of bond force constants and the equilibrium configuration of atomic coordinates predicted by DFT as the input geometry for FEA improves its predictions. The significance of the numerical values chosen for the bond force constants in FEA is also discussed.

quote

GB/T 7714-2015 [1] G. DomínguezRodríguez, A. Tapia, F. Avilés. Computational Materials Science, 2014(82). DOI:10.1016/j.commatsci.2013.10.003.
MLA [1] G. DomínguezRodríguez, et al., Computational Materials Science, no. 82, 2014, https://doi.org/10.1016/j.commatsci.2013.10.003.
APA [1] G. DomínguezRodríguez, A. Tapia, & F. Avilés. (2014). Computational Materials Science(82). https://doi.org/10.1016/j.commatsci.2013.10.003
IEEE [1] G. DomínguezRodríguez, A. Tapia, and F. Avilés, Computational Materials Science, no. 82, 2014, doi: 10.1016/j.commatsci.2013.10.003.