Upcycling Fabrics: Valorization of Recycled Polyethylene Terephthalate (r-PET) Plastic Waste into Thermoplastic Polyester Elastomers (TPEE) for Fiber Spinning AITranslate
Abstract AITranslate
Plastic waste has been one of the major sources of pollution in landfills and oceans. Although the upcycling of polymers has been proposed as a sustainable solution, multifunctional fibers based on upcycling concepts still require further investigation, which can extend the applications of environmentally friendly materials. In this work, we present an interesting strategy for fabricating stretchable, flexible, and durable fabrics via “up-polymerization” and electrospinning. Recycled polyethylene terephthalate (r-PET) waste films are converted to upcycled thermoplastic polyester elastomers (TPEE, PBT-co-PTMEG) via an esterification reaction and condensation polymerization. After dissolution in a trifluoroacetic acid (TFA)/dichloromethane (DCM) binary solvent system, the upcycled TPEE is electrospun into aligned fibrous membranes using a rotating drum. By adjusting the volume ratios of TFA/DCM or the polymer concentration, the diameters of the fibers can be controlled. Furthermore, the mechanical properties of the upcycled TPEE fabrics are determined by tensile measurement tests. The stress–strain curves show that the upcycled TPEE membranes exhibit good flexibility compared to commercial TPEE membranes. Moreover, the upcycled TPEE fabrics demonstrate excellent elastic recovery during cyclic tensile tests.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c01943
Chinese Library Classification Number:
Citation Information:
Plastic waste has been one of the major sources of pollution in landfills and oceans. Although the upcycling of polymers has been proposed as a sustainable solution, multifunctional fibers based on upcycling concepts still require further investigation, which can extend the applications of environmentally friendly materials. In this work, we present an interesting strategy for fabricating stretchable, flexible, and durable fabrics via “up-polymerization” and electrospinning. Recycled polyethylene terephthalate (r-PET) waste films are converted to upcycled thermoplastic polyester elastomers (TPEE, PBT-co-PTMEG) via an esterification reaction and condensation polymerization. After dissolution in a trifluoroacetic acid (TFA)/dichloromethane (DCM) binary solvent system, the upcycled TPEE is electrospun into aligned fibrous membranes using a rotating drum. By adjusting the volume ratios of TFA/DCM or the polymer concentration, the diameters of the fibers can be controlled. Furthermore, the mechanical properties of the upcycled TPEE fabrics are determined by tensile measurement tests. The stress–strain curves show that the upcycled TPEE membranes exhibit good flexibility compared to commercial TPEE membranes. Moreover, the upcycled TPEE fabrics demonstrate excellent elastic recovery during cyclic tensile tests.
quote
| GB/T 7714-2015 | [1] JhihHao Ho, KaiChuan Kuo, TseYu Lo, et al. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c01943. |
| MLA | [1] JhihHao Ho, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c01943. |
| APA | [1] JhihHao Ho, KaiChuan Kuo, TseYu Lo, ChunTing Chang, YuHsuan Tseng, Bhaskarchand Gautam, CheTseng Lin, & JiunTai Chen. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c01943 |
| IEEE | [1] JhihHao Ho, KaiChuan Kuo, TseYu Lo, ChunTing Chang, YuHsuan Tseng, Bhaskarchand Gautam, CheTseng Lin, and JiunTai Chen, ACS Applied Polymer Materials, no. 6, 2024, doi: 10.1021/acsapm.3c01943. keywords: {polymer upcycling;thermoplastic polyester elastomers;polyethylene terephthalate;cyclic test;electrospinning} |