daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Synthesis and Characterization of Sulfur-Based Polymers from Elemental Sulfur and Algae Oil AITranslate

University of Tsukuba; University of Tsukuba; University of Tsukuba;Samsung R&D Institute Japan;Samsung R&D Institute Japan;National Institute of Advanced Industrial Science and Technology (AIST);National Institute of Advanced Industrial Science and Technology (AIST);National Institute of Advanced Industrial Science and Technology (AIST); University of Tsukuba; University of Tsukuba
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Sulfur-based polymeric materials were obtained from surplus feedstock; elemental sulfur; and sustainable algae oil, Botryococcene, via inverse vulcanization. Reactions of elemental sulfur and Botryococcene at 185 °C produce polymeric materials with various weight ratios of sulfur and Botryococcene (5:5 to 9:1), depending on the feed ratio. In this study, these polymers have been characterized from several aspects using spectral analysis, thermoanalysis, and electrochemical analysis. When the composition of sulfur is more than 70 wt %, the polymer contains a residual sulfur element not incorporated in the polymer chains. The sulfur-based polymers can be pressed into intended shapes when heated at 120 °C. The polymers could serve as active materials for Li–S batteries. This investigation of structure and properties provides basic information for future applications.

KeyWords AITranslate

algae biomass sulfur inverse vulcanization Li−S battery Botryococcene
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00197

Chinese Library Classification Number:

Citation Information:

Sulfur-based polymeric materials were obtained from surplus feedstock; elemental sulfur; and sustainable algae oil, Botryococcene, via inverse vulcanization. Reactions of elemental sulfur and Botryococcene at 185 °C produce polymeric materials with various weight ratios of sulfur and Botryococcene (5:5 to 9:1), depending on the feed ratio. In this study, these polymers have been characterized from several aspects using spectral analysis, thermoanalysis, and electrochemical analysis. When the composition of sulfur is more than 70 wt %, the polymer contains a residual sulfur element not incorporated in the polymer chains. The sulfur-based polymers can be pressed into intended shapes when heated at 120 °C. The polymers could serve as active materials for Li–S batteries. This investigation of structure and properties provides basic information for future applications.

quote

GB/T 7714-2015 [1] Shuhei Oishi, Kaho Oi, Junpei Kuwabara, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00197.
MLA [1] Shuhei Oishi, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00197.
APA [1] Shuhei Oishi, Kaho Oi, Junpei Kuwabara, Ryo Omoda, Yuichi Aihara, Takashi Fukuda, Toshikazu Takahashi, JunChul Choi, Makoto Watanabe, & Takaki Kanbara. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00197
IEEE [1] Shuhei Oishi, Kaho Oi, Junpei Kuwabara, Ryo Omoda, Yuichi Aihara, Takashi Fukuda, Toshikazu Takahashi, JunChul Choi, Makoto Watanabe, and Takaki Kanbara, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00197. keywords: {algae biomass;sulfur;inverse vulcanization;Li−S battery;Botryococcene}