daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Critical assessment of the Ag–Bi–Sn ternary system AITranslate

Institute of Metallurgy and Materials Science;Institute of Metallurgy and Materials Science
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A history of system assessments was given, and all the experimental works on its thermodynamics and constitution were mentioned, as well. A dataset for preliminary optimization was constructed, all existing phases of ternary system were listed and appropriate thermodynamic models were chosen. Optimization was carried out in the subsequent steps, and ternary thermodynamic parameters of all the phases under accord were determined. Equilibrium calculations resulted in phase boundary coordinates, invariant reaction parameters and thermodynamic function values; a Scheil reaction scheme was constructed, as well. Calculated quantities were then compared to the existing experimental data displaying the excellent agreement. Suggestion on the choice of alloy compositions was given as for solder material.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.calphad.2008.07.001

Chinese Library Classification Number:

Citation Information:

A history of system assessments was given, and all the experimental works on its thermodynamics and constitution were mentioned, as well. A dataset for preliminary optimization was constructed, all existing phases of ternary system were listed and appropriate thermodynamic models were chosen. Optimization was carried out in the subsequent steps, and ternary thermodynamic parameters of all the phases under accord were determined. Equilibrium calculations resulted in phase boundary coordinates, invariant reaction parameters and thermodynamic function values; a Scheil reaction scheme was constructed, as well. Calculated quantities were then compared to the existing experimental data displaying the excellent agreement. Suggestion on the choice of alloy compositions was given as for solder material.

quote

GB/T 7714-2015 [1] Leszek A. Zabdyr, G. Garzeł. Calphad, 2009(33). DOI:10.1016/j.calphad.2008.07.001.
MLA [1] Leszek A. Zabdyr, and G. Garzeł. Calphad, no. 33, 2009, https://doi.org/10.1016/j.calphad.2008.07.001.
APA [1] Leszek A. Zabdyr, & G. Garzeł. (2009). Calphad(33). https://doi.org/10.1016/j.calphad.2008.07.001
IEEE [1] Leszek A. Zabdyr and G. Garzeł, Calphad, no. 33, 2009, doi: 10.1016/j.calphad.2008.07.001.