Fluorescent Patterns by Selective Grafting of a Telechelic Polymer AITranslate
Abstract AITranslate
The preparation of patterned ultrathin films (sub-10 nm) composed of end-anchored fluorescently labeled poly(methyl methacrylate) (PMMA) is presented. Telechelic PMMA was synthesized utilizing activator regenerated by electron transfer atom transfer radical polymerization and consecutively end-functionalized with alkynylated fluorescein by Cu-catalyzed azide–alkyne cycloaddition (CuAAC) “click” chemistry. The polymers were grafted via the α-carboxyl groups to silica or glass substrates pretreated with (3-aminopropyl)triethoxysilane (APTES). Patterned surfaces were prepared by inkjet printing of APTES onto glass substrates and selectively grafted with fluorescently end-labeled PMMA to obtain emissive arrays on the surface.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.8b00180
Chinese Library Classification Number:
Citation Information:
The preparation of patterned ultrathin films (sub-10 nm) composed of end-anchored fluorescently labeled poly(methyl methacrylate) (PMMA) is presented. Telechelic PMMA was synthesized utilizing activator regenerated by electron transfer atom transfer radical polymerization and consecutively end-functionalized with alkynylated fluorescein by Cu-catalyzed azide–alkyne cycloaddition (CuAAC) “click” chemistry. The polymers were grafted via the α-carboxyl groups to silica or glass substrates pretreated with (3-aminopropyl)triethoxysilane (APTES). Patterned surfaces were prepared by inkjet printing of APTES onto glass substrates and selectively grafted with fluorescently end-labeled PMMA to obtain emissive arrays on the surface.
quote
| GB/T 7714-2015 | [1] Maciej Kopeć, Sinem Tas, Marco Cirelli, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.8b00180. |
| MLA | [1] Maciej Kopeć, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.8b00180. |
| APA | [1] Maciej Kopeć, Sinem Tas, Marco Cirelli, Rianne van der Pol, Ilse de Vries, G. Julius Vancso, & Sissi de Beer. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.8b00180 |
| IEEE | [1] Maciej Kopeć, Sinem Tas, Marco Cirelli, Rianne van der Pol, Ilse de Vries, G. Julius Vancso, and Sissi de Beer, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.8b00180. keywords: {grafting to;inkjet printing;polymer brushes;ATRP;click chemistry} |