daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Fabrication and Properties of Anti-freezing Gelatin Hydrogels Based on a Deep Eutectic Solvent AITranslate

Qilu University of Technology (Shandong Academy of Sciences); Qilu University of Technology (Shandong Academy of Sciences); Qilu University of Technology (Shandong Academy of Sciences); Qilu University of Technology (Shandong Academy of Sciences); Qilu University of Technology (Shandong Academy of Sciences)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In this study, gelatin hydrogels with excellent anti-freezing properties were prepared by simply immersing the initial hydrogels in a deep eutectic solvent (DES) aqueous solution. The formation of ice crystals in hydrogels is greatly hindered by introduction of the DES even at very low temperatures. The hydrogels still remain mechanically flexible even at −80 °C. In addition, the DES could facilitate the protein chain bundling, resulting in the formation of triple helices and thus improving the mechanical properties of gelatin hydrogels. Furthermore, the hydrogels could be stored for a long time with slight water loss, thus showing good water retention performance.

KeyWords AITranslate

gelatin deep eutectic solvent soaking method antifreezing hydrogen bonding
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00634

Chinese Library Classification Number:

Citation Information:

In this study, gelatin hydrogels with excellent anti-freezing properties were prepared by simply immersing the initial hydrogels in a deep eutectic solvent (DES) aqueous solution. The formation of ice crystals in hydrogels is greatly hindered by introduction of the DES even at very low temperatures. The hydrogels still remain mechanically flexible even at −80 °C. In addition, the DES could facilitate the protein chain bundling, resulting in the formation of triple helices and thus improving the mechanical properties of gelatin hydrogels. Furthermore, the hydrogels could be stored for a long time with slight water loss, thus showing good water retention performance.

quote

GB/T 7714-2015 [1] Runpeng Liu, Congde Qiao, Qinze Liu, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00634.
MLA [1] Runpeng Liu, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00634.
APA [1] Runpeng Liu, Congde Qiao, Qinze Liu, Libin Liu, & Jinshui Yao. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00634
IEEE [1] Runpeng Liu, Congde Qiao, Qinze Liu, Libin Liu, and Jinshui Yao, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00634. keywords: {gelatin;deep eutectic solvent;soaking method;antifreezing;hydrogen bonding}