daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Hydroxytyrosol: Bioinspired Nature-Based Adhesive Motif with Excellent Chemical Modifiability and Stability AITranslate

University of Tsukuba; National Institute for Materials Science (NIMS);Osaka Research Institute of Industrial Science and Technology; University of Tsukuba
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Dopamine and its derivatives have been discovered as biomimetic adhesive motifs for various applications, but their affordability has been an obstacle to their practical realization. To address both high performance and productivity, we propose hydroxytyrosol as a nature-based adhesive motif. The productivity of hydroxytyrosol was overcome by the biosynthesis of hydroxytyrosol using glucose as the starting material. Because hydroxytyrosol is not easily autoxidized, hydroxytyrosol can be introduced into alkyl methacrylate through an unprotected one-pot transesterification reaction. The resulting adhesive copolymers with hydroxytyrosol as a side chain show adhesive properties comparable to those of the corresponding dopamine-containing polymers.

KeyWords AITranslate

hydroxytyrosol mussel adhesion 3 4dihydroxyphenyllalanine bioinspired material
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00365

Chinese Library Classification Number:

Citation Information:

Dopamine and its derivatives have been discovered as biomimetic adhesive motifs for various applications, but their affordability has been an obstacle to their practical realization. To address both high performance and productivity, we propose hydroxytyrosol as a nature-based adhesive motif. The productivity of hydroxytyrosol was overcome by the biosynthesis of hydroxytyrosol using glucose as the starting material. Because hydroxytyrosol is not easily autoxidized, hydroxytyrosol can be introduced into alkyl methacrylate through an unprotected one-pot transesterification reaction. The resulting adhesive copolymers with hydroxytyrosol as a side chain show adhesive properties comparable to those of the corresponding dopamine-containing polymers.

quote

GB/T 7714-2015 [1] Takehiro Fujita, Eri Nishi, Daisuke Koma, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00365.
MLA [1] Takehiro Fujita, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00365.
APA [1] Takehiro Fujita, Eri Nishi, Daisuke Koma, & Masanobu Naito. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00365