Engineering Materials for Progressive All-Solid-State Na Batteries AITranslate
Abstract AITranslate
Following the prevalence of the Li-ion battery for electrical energy storage systems (EESs), the world is looking toward alternative, cost-effective, electrical EESs for portable electronics, electric vehicles, and grid storage from renewable sources. Na-based batteries are the most promising candidates and show similar chemistry as Li-based batteries. All-solid-state sodium batteries (AS3Bs) have attracted great attention due to safe operation, high energy density, and wide operational temperature. Herein, current development of solid-state crystalline borate- and chalcogenide-based Na-ion conductors is discussed together with historically important Na-β-alumina and Na superionic conductors (NASICONs). Furthermore, we report on engineering a ceramic Na-ion electrolyte and electrode interface, which is considered a bottleneck for practical applications of solid-state electrolytes in AS3Bs. A soft Na-ion conducting interlayer is critical to suppress the interfacial Na-ion charge transfer resistance between the solid electrolyte and electrode. Several Na-ion conducting ionic liquids, polymers, gels, crystalline plastics interlayers, and other interfacial modification strategies have been effectively employed in advanced AS3Bs.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.8b00948
Chinese Library Classification Number:
Citation Information:
Following the prevalence of the Li-ion battery for electrical energy storage systems (EESs), the world is looking toward alternative, cost-effective, electrical EESs for portable electronics, electric vehicles, and grid storage from renewable sources. Na-based batteries are the most promising candidates and show similar chemistry as Li-based batteries. All-solid-state sodium batteries (AS3Bs) have attracted great attention due to safe operation, high energy density, and wide operational temperature. Herein, current development of solid-state crystalline borate- and chalcogenide-based Na-ion conductors is discussed together with historically important Na-β-alumina and Na superionic conductors (NASICONs). Furthermore, we report on engineering a ceramic Na-ion electrolyte and electrode interface, which is considered a bottleneck for practical applications of solid-state electrolytes in AS3Bs. A soft Na-ion conducting interlayer is critical to suppress the interfacial Na-ion charge transfer resistance between the solid electrolyte and electrode. Several Na-ion conducting ionic liquids, polymers, gels, crystalline plastics interlayers, and other interfacial modification strategies have been effectively employed in advanced AS3Bs.
quote
| GB/T 7714-2015 | [1] Chengtian Zhou, Sourav Bag, Venkataraman Thangadurai. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00948. |
| MLA | [1] Chengtian Zhou, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00948. |
| APA | [1] Chengtian Zhou, Sourav Bag, & Venkataraman Thangadurai. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00948 |
| IEEE | [1] Chengtian Zhou, Sourav Bag, and Venkataraman Thangadurai, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00948. |