Achieving Higher Dielectric and Energy Storage Performances of Methyl Methacrylate-co-glycidyl Methacrylate Films through the Nanocomposite Strategy AITranslate

Changchun University of Technology; Changchun University of Technology; Changchun University of Technology; Changchun University of Technology; Changchun University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Polymer-based nanocomposite dielectric films with excellent breakdown strength and high discharged energy density are desired for advanced dielectric film capacitors. Herein, a series of methyl methacrylate (MMA) and glycidyl methacrylate (GMA) copolymer (MG) nanocomposite films with organic montmorillonite (OMMT) as a modifier were prepared by a solution-processed method. Density functional theory proved that the introduction of GMA groups in the MG copolymer effectively formed deep energy traps, which were beneficial to free carrier capture, weak leakage current density, and high breakdown strength. The introduction of the 2D OMMT nanosheets further improved the dielectric constant of the MG copolymer through interfacial polarization. In addition, the formation of nano interfaces between MG and OMMT also provided deep traps, which limited charge injection and migration, resulting in lower dielectric/conductive losses and higher breakdown strength. Meanwhile, the addition of OMMT hindered further extension of electrical trees in the nanocomposite films due to the 2D structure according to finite element simulation. The energy storage results indicated that the MG/OMMT nanocomposite film with 1 wt % OMMT concentration achieved a 780 MV/m breakdown strength, 10.95 J/cm3 discharged energy density, and 85% energy efficiency. Therefore, this research provides a simple and feasible strategy for the manufacture of thin-film capacitors.

KeyWords AITranslate

MG copolymer OMMT nanocomposite dielectric films deep traps energy storage
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01504

Chinese Library Classification Number:

Citation Information:

Polymer-based nanocomposite dielectric films with excellent breakdown strength and high discharged energy density are desired for advanced dielectric film capacitors. Herein, a series of methyl methacrylate (MMA) and glycidyl methacrylate (GMA) copolymer (MG) nanocomposite films with organic montmorillonite (OMMT) as a modifier were prepared by a solution-processed method. Density functional theory proved that the introduction of GMA groups in the MG copolymer effectively formed deep energy traps, which were beneficial to free carrier capture, weak leakage current density, and high breakdown strength. The introduction of the 2D OMMT nanosheets further improved the dielectric constant of the MG copolymer through interfacial polarization. In addition, the formation of nano interfaces between MG and OMMT also provided deep traps, which limited charge injection and migration, resulting in lower dielectric/conductive losses and higher breakdown strength. Meanwhile, the addition of OMMT hindered further extension of electrical trees in the nanocomposite films due to the 2D structure according to finite element simulation. The energy storage results indicated that the MG/OMMT nanocomposite film with 1 wt % OMMT concentration achieved a 780 MV/m breakdown strength, 10.95 J/cm3 discharged energy density, and 85% energy efficiency. Therefore, this research provides a simple and feasible strategy for the manufacture of thin-film capacitors.

quote

GB/T 7714-2015 [1] Junhao Xie, Hongxu Liu, Xuanchen Zhao, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01504.
MLA [1] Junhao Xie, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01504.
APA [1] Junhao Xie, Hongxu Liu, Xuanchen Zhao, Shulin Sun, & Mingyao Zhang. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01504
IEEE [1] Junhao Xie, Hongxu Liu, Xuanchen Zhao, Shulin Sun, and Mingyao Zhang, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01504. keywords: {MG copolymer;OMMT;nanocomposite dielectric films;deep traps;energy storage}