Thermodynamic modeling of the Mo–Pt system based on the NACEF approach AITranslate
Abstract AITranslate
The present work reports on a thermodynamic modeling of the Mo–Pt system using a combined first-principles/CALPHAD approach. First-Principles (FP) calculations are performed to obtain the enthalpies of formation for the four ordered phases of the system (A15, B19, D019 and MoPt2) at 0 K. The liquid, bcc, fcc and hcp phases have been modeled as substitutional solutions where the excess term is in the form of the Redlich–Kister polynomial. The four ordered phases are modeled using the NACEF approach taking into account the three order-disorder transitions (B19/A3, D019/A3 and MoPt2/A1). FP calculations, experimental phase equilibria and site occupancies data are used to evaluate the model parameters. The thermodynamic description of the Mo–Pt system obtained in this work agree well with all the available data with a limited number of parameters used.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.calphad.2024.102665
Chinese Library Classification Number:
Citation Information:
The present work reports on a thermodynamic modeling of the Mo–Pt system using a combined first-principles/CALPHAD approach. First-Principles (FP) calculations are performed to obtain the enthalpies of formation for the four ordered phases of the system (A15, B19, D019 and MoPt2) at 0 K. The liquid, bcc, fcc and hcp phases have been modeled as substitutional solutions where the excess term is in the form of the Redlich–Kister polynomial. The four ordered phases are modeled using the NACEF approach taking into account the three order-disorder transitions (B19/A3, D019/A3 and MoPt2/A1). FP calculations, experimental phase equilibria and site occupancies data are used to evaluate the model parameters. The thermodynamic description of the Mo–Pt system obtained in this work agree well with all the available data with a limited number of parameters used.
quote
| GB/T 7714-2015 | [1] J.M. Fiorani, M. Siblani, J.M. Joubert, et al. Calphad, 2024(84). DOI:10.1016/j.calphad.2024.102665. |
| MLA | [1] J.M. Fiorani, et al., Calphad, no. 84, 2024, https://doi.org/10.1016/j.calphad.2024.102665. |
| APA | [1] J.M. Fiorani, M. Siblani, J.M. Joubert, C. Barreteau, J.C. Crivello, N. David, & M. Vilasi. (2024). Calphad(84). https://doi.org/10.1016/j.calphad.2024.102665 |
| IEEE | [1] J.M. Fiorani, M. Siblani, J.M. Joubert, C. Barreteau, J.C. Crivello, N. David, and M. Vilasi, Calphad, no. 84, 2024, doi: 10.1016/j.calphad.2024.102665. |