Realizing Dynamic Diffraction Gratings Based on Light-Direct Writing of Responsive 2D Ordered Patterns AITranslate

Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A dynamic diffraction grating (DDG) can realize on-demand in-situ regulation of light diffraction and is highly necessary in the next-generation optical devices; however, its fabrication remains challenging because of difficulties in generating a responsive pattern in the bulk material or on the surface. In this study, a facile and general approach to construct DDG is developed based on the near-infrared radiation (NIR)-driven responsive 2D ordered surface pattern, which is fabricated by light-direct writing of wrinkles on a thin film of a photosensitive supramolecular polymer network comprised of a copolymer containing amino groups, anthracene carboxylic acid (ANA), and carbon nanotubes. The resulting surface pattern, which exhibits a height dependence on the NIR irradiation, can be used as the DDG whose optical diffraction can be regulated in-situ by NIR. Furthermore, because of the presence of a reversible ANA photodimer and hydrogen bonding in the supramolecular network, the patterned surface can be erased and rewritten by UV light with different wavelengths and self-healed by NIR irradiation. The results demonstrate a simple strategy for DDGs that will have a broad application in the fields of optics, electronics, and intelligent sensing.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.0c00285

Chinese Library Classification Number:

Citation Information:

A dynamic diffraction grating (DDG) can realize on-demand in-situ regulation of light diffraction and is highly necessary in the next-generation optical devices; however, its fabrication remains challenging because of difficulties in generating a responsive pattern in the bulk material or on the surface. In this study, a facile and general approach to construct DDG is developed based on the near-infrared radiation (NIR)-driven responsive 2D ordered surface pattern, which is fabricated by light-direct writing of wrinkles on a thin film of a photosensitive supramolecular polymer network comprised of a copolymer containing amino groups, anthracene carboxylic acid (ANA), and carbon nanotubes. The resulting surface pattern, which exhibits a height dependence on the NIR irradiation, can be used as the DDG whose optical diffraction can be regulated in-situ by NIR. Furthermore, because of the presence of a reversible ANA photodimer and hydrogen bonding in the supramolecular network, the patterned surface can be erased and rewritten by UV light with different wavelengths and self-healed by NIR irradiation. The results demonstrate a simple strategy for DDGs that will have a broad application in the fields of optics, electronics, and intelligent sensing.

quote

GB/T 7714-2015 [1] Luzhi Zhang, Guotao Sun, Jing Bai, et al. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.0c00285.
MLA [1] Luzhi Zhang, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.0c00285.
APA [1] Luzhi Zhang, Guotao Sun, Jing Bai, Xiaodong Ma, Jie Yin, Qingkang Wang, & Xuesong Jiang. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.0c00285
IEEE [1] Luzhi Zhang, Guotao Sun, Jing Bai, Xiaodong Ma, Jie Yin, Qingkang Wang, and Xuesong Jiang, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.0c00285.