daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Demonstration of High Detoxification Efficiency of Glassy Polymer–Metal Hydroxide Composites toward Chemical Warfare Agent Simulants AITranslate

Missouri University of Science and Technology; Missouri University of Science and Technology; Missouri University of Science and Technology; Cleveland State University; Missouri University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The design and development of polymeric composites that can effectively capture and destruct toxic chemicals with a fast detoxification rate is of high importance for protecting the military, first responders, and civilians. Here we report the synthesis and assessment of zirconium hydroxide (Zr(OH)4)-incorporated Ultem, Matrimid, and PIM-1 composites for detoxification of dimethyl 4-nitrophenylphosphonate (DMNP), as a type G toxic nerve agent simulant. Maintaining homogeneity, three different loadings (8, 20, 30 wt %) of Zr(OH)4 were incorporated into the polymers, and the thin films of composite materials were developed for subsequent hydrolysis tests. Our results indicated that increasing the Zr(OH)4 loading enhances the hydrolysis rate and the amount of DMNP converted for all three polymers. While the surface area and porosity of PIM-1 reduced upon increasing Zr(OH)4 loading, 30%-Zr(OH)4@PIM-1 was found to be the best performing material to achieve ∼100% conversion in 2 h with a hydrolysis rate of 5.5 × 10–3 μmol/s at room temperature. It was also observed that the performance of 30%-Zr(OH)4@PIM-1 is drastically improved at 60 °C by exhibiting a conversion rate of 4.9 μmol/s, while achieving 100% conversion almost instantaneously (within 5 s). Our findings represent a substantial improvement of this class of materials over previously reported polymer-metalhydroxide composites toward the detoxification of toxic gases.

KeyWords AITranslate

detoxification chemical warfare agent hydrolysis composites polymer
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00918

Chinese Library Classification Number:

Citation Information:

The design and development of polymeric composites that can effectively capture and destruct toxic chemicals with a fast detoxification rate is of high importance for protecting the military, first responders, and civilians. Here we report the synthesis and assessment of zirconium hydroxide (Zr(OH)4)-incorporated Ultem, Matrimid, and PIM-1 composites for detoxification of dimethyl 4-nitrophenylphosphonate (DMNP), as a type G toxic nerve agent simulant. Maintaining homogeneity, three different loadings (8, 20, 30 wt %) of Zr(OH)4 were incorporated into the polymers, and the thin films of composite materials were developed for subsequent hydrolysis tests. Our results indicated that increasing the Zr(OH)4 loading enhances the hydrolysis rate and the amount of DMNP converted for all three polymers. While the surface area and porosity of PIM-1 reduced upon increasing Zr(OH)4 loading, 30%-Zr(OH)4@PIM-1 was found to be the best performing material to achieve ∼100% conversion in 2 h with a hydrolysis rate of 5.5 × 10–3 μmol/s at room temperature. It was also observed that the performance of 30%-Zr(OH)4@PIM-1 is drastically improved at 60 °C by exhibiting a conversion rate of 4.9 μmol/s, while achieving 100% conversion almost instantaneously (within 5 s). Our findings represent a substantial improvement of this class of materials over previously reported polymer-metalhydroxide composites toward the detoxification of toxic gases.

quote

GB/T 7714-2015 [1] Peter O. Aina, Sukanta K. Mondal, Joshua Costain, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00918.
MLA [1] Peter O. Aina, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00918.
APA [1] Peter O. Aina, Sukanta K. Mondal, Joshua Costain, Ali A. Rownaghi, & Fateme Rezaei. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00918
IEEE [1] Peter O. Aina, Sukanta K. Mondal, Joshua Costain, Ali A. Rownaghi, and Fateme Rezaei, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00918. keywords: {detoxification;chemical warfare agent;hydrolysis;composites;polymer}