Molecularly Designing a Passivation ETL to Suppress EQE Roll-off of PeLEDs AITranslate
Abstract AITranslate
Efficiently suppressing the external quantum efficiency (EQE) roll-off of perovskite light-emitting diodes (PeLEDs) urgently requires designing passivation electron transporting layers (ETLs) for intrinsically passivating perovskite surface defects toward next-generation illumination and display. Here, we molecularly designed the inherent passivation ETL B3PyPPM with a strong nucleophilic core-group to effectively passivate perovskite surface defects. Compared with ETL B3PyMPM, the B3PyPPM can theoretically form a tighter interaction with the perovskite surface and transfer more electrons to better passivate surface Pb2+ vacancies, leading to superior suppression of EQE roll-off in PeLEDs by reducing the trap-assisted nonradiative recombination. Experimentally, the B3PyPPM-based PeLED exhibits a higher EQE of 18.04%, greater luminance of 4.15 times, and a longer T50 of 5.38 times than B3PyMPM-based PeLEDs, evidently proving the superior EQE roll-off suppression of the stronger nucleophilic core-group-based ETL. Therefore, this work provides important guidance for rationally designing multifunctional ETLs to achieve high-performance and long-term stability in PeLEDs.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.3c01379
Chinese Library Classification Number:
Citation Information:
Efficiently suppressing the external quantum efficiency (EQE) roll-off of perovskite light-emitting diodes (PeLEDs) urgently requires designing passivation electron transporting layers (ETLs) for intrinsically passivating perovskite surface defects toward next-generation illumination and display. Here, we molecularly designed the inherent passivation ETL B3PyPPM with a strong nucleophilic core-group to effectively passivate perovskite surface defects. Compared with ETL B3PyMPM, the B3PyPPM can theoretically form a tighter interaction with the perovskite surface and transfer more electrons to better passivate surface Pb2+ vacancies, leading to superior suppression of EQE roll-off in PeLEDs by reducing the trap-assisted nonradiative recombination. Experimentally, the B3PyPPM-based PeLED exhibits a higher EQE of 18.04%, greater luminance of 4.15 times, and a longer T50 of 5.38 times than B3PyMPM-based PeLEDs, evidently proving the superior EQE roll-off suppression of the stronger nucleophilic core-group-based ETL. Therefore, this work provides important guidance for rationally designing multifunctional ETLs to achieve high-performance and long-term stability in PeLEDs.
quote
| GB/T 7714-2015 | [1] Qungui Wang, Yongjian Chen, Cheng Yan, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c01379. |
| MLA | [1] Qungui Wang, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c01379. |
| APA | [1] Qungui Wang, Yongjian Chen, Cheng Yan, Xiankan Zeng, Xuehai Fu, Lunyao Pan, Jingjing Cao, Shiyu Yang, Wen Li, Xiangrong Chen, & Weiqing Yang. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c01379 |
| IEEE | [1] Qungui Wang, Yongjian Chen, Cheng Yan, Xiankan Zeng, Xuehai Fu, Lunyao Pan, Jingjing Cao, Shiyu Yang, Wen Li, Xiangrong Chen, and Weiqing Yang, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c01379. |