daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Toughening Poly(lactide) with Bio-Based Poly(farnesene) Elastomers AITranslate

3610 University Street; McGill University; 3610 University Street; 3610 University Street
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The development and application of bio-sourced elastomers which can be blended with poly(lactide) (PLA) to enhance its poor material properties are of great interest as we move toward replacing petroleum-derived plastics with viable alternatives. As such, this work focused on the valorization of the terpene-based monomer, trans-β-farnesene (farnesene), as a building block to design rubber toughening agents to improve the impact strength of PLA blends. Ternary blends consisting of copolymers of farnesene–glycidyl methacrylate (PFGMA), farnesene–methacrylic acid (PFMAA) (20–30 wt % farnesene copolymers), and PLA exhibited significant improvements in impact strength and elongation at break (i.e., approximately 16-fold and 10-fold, respectively) over neat PLA. Torque mixer measurements and FTIR spectroscopy confirmed the occurrence of epoxy–acid/epoxy–hydroxyl interfacial compatibilization reactions catalyzed through hydrogen-bonding interactions. Phase morphologies of the ternary blends were evaluated with scanning electron microscopy (SEM) and showed an approximate 4-fold reduction in particle diameter relative to the binary systems (i.e., from 4.3 to 1.1 μm) with the compatibilized blend morphology deemed stable upon annealing. The toughening mechanism responsible for the improved mechanical properties observed with the ternary blends was also investigated by examining the impact fractured surface morphologies with SEM. A combination of enhanced interfacial adhesion coupled with shear yielding of the matrix was proposed as the main contributing factor to the improvement in mechanical properties observed in the ternary blends.

KeyWords AITranslate

poly(lactide) biobased elastomer toughening ternary blend reactive blending
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01183

Chinese Library Classification Number:

Citation Information:

The development and application of bio-sourced elastomers which can be blended with poly(lactide) (PLA) to enhance its poor material properties are of great interest as we move toward replacing petroleum-derived plastics with viable alternatives. As such, this work focused on the valorization of the terpene-based monomer, trans-β-farnesene (farnesene), as a building block to design rubber toughening agents to improve the impact strength of PLA blends. Ternary blends consisting of copolymers of farnesene–glycidyl methacrylate (PFGMA), farnesene–methacrylic acid (PFMAA) (20–30 wt % farnesene copolymers), and PLA exhibited significant improvements in impact strength and elongation at break (i.e., approximately 16-fold and 10-fold, respectively) over neat PLA. Torque mixer measurements and FTIR spectroscopy confirmed the occurrence of epoxy–acid/epoxy–hydroxyl interfacial compatibilization reactions catalyzed through hydrogen-bonding interactions. Phase morphologies of the ternary blends were evaluated with scanning electron microscopy (SEM) and showed an approximate 4-fold reduction in particle diameter relative to the binary systems (i.e., from 4.3 to 1.1 μm) with the compatibilized blend morphology deemed stable upon annealing. The toughening mechanism responsible for the improved mechanical properties observed with the ternary blends was also investigated by examining the impact fractured surface morphologies with SEM. A combination of enhanced interfacial adhesion coupled with shear yielding of the matrix was proposed as the main contributing factor to the improvement in mechanical properties observed in the ternary blends.

quote

GB/T 7714-2015 [1] Matthew W. Halloran, Jim A. Nicell, Richard L. Leask, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01183.
MLA [1] Matthew W. Halloran, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01183.
APA [1] Matthew W. Halloran, Jim A. Nicell, Richard L. Leask, & Milan Marić. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01183
IEEE [1] Matthew W. Halloran, Jim A. Nicell, Richard L. Leask, and Milan Marić, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01183. keywords: {poly(lactide);biobased elastomer;toughening;ternary blend;reactive blending}