Tuning Size and Seed Position in Small Silver Nanorods AITranslate

CIC biomaGUNE, Basque Research and Technology Alliance (BRTA);CIC biomaGUNE, Basque Research and Technology Alliance (BRTA); University of Antwerp; University of Antwerp;CIC biomaGUNE, Basque Research and Technology Alliance (BRTA)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Although high-quality gold nanorods can be routinely synthesized, within a wide range of sizes and aspect ratios, a similar level of control has not been reached for silver nanorods. Whereas seeded-growth processes have been developed, the reported methods have not met sufficient interest, mainly because of limited quality, particularly when small size (short diameter) and small aspect ratios are targeted. In the surfactant-driven seeded growth of gold nanorods, the success of the synthesis is largely dependent on the quality and stability of the seeds, and thus related methods have been reported for the seeded growth of Ag nanorods, using penta-twinned Au nanorods and bipyramids as seeds. However, Ag nanorods with diameters of >30 nm are consistently obtained, restricting their potential applications. We report the preparation of high-quality silver nanorods, using either small bipyramids or small decahedra as seeds, with special attention to the location of the seeds, either at the center (bipyramids) or at one end (decahedra) of the resulting nanorods.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.0c00388

Chinese Library Classification Number:

Citation Information:

Although high-quality gold nanorods can be routinely synthesized, within a wide range of sizes and aspect ratios, a similar level of control has not been reached for silver nanorods. Whereas seeded-growth processes have been developed, the reported methods have not met sufficient interest, mainly because of limited quality, particularly when small size (short diameter) and small aspect ratios are targeted. In the surfactant-driven seeded growth of gold nanorods, the success of the synthesis is largely dependent on the quality and stability of the seeds, and thus related methods have been reported for the seeded growth of Ag nanorods, using penta-twinned Au nanorods and bipyramids as seeds. However, Ag nanorods with diameters of >30 nm are consistently obtained, restricting their potential applications. We report the preparation of high-quality silver nanorods, using either small bipyramids or small decahedra as seeds, with special attention to the location of the seeds, either at the center (bipyramids) or at one end (decahedra) of the resulting nanorods.

quote

GB/T 7714-2015 [1] Ana SánchezIglesias, Xiaolu Zhuo, Wiebke Albrecht, et al. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.0c00388.
MLA [1] Ana SánchezIglesias, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.0c00388.
APA [1] Ana SánchezIglesias, Xiaolu Zhuo, Wiebke Albrecht, Sara Bals, & Luis M. LizMarzán. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.0c00388
IEEE [1] Ana SánchezIglesias, Xiaolu Zhuo, Wiebke Albrecht, Sara Bals, and Luis M. LizMarzán, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.0c00388.