Multispectral Thermal Management Designs for Net-Zero Energy Buildings AITranslate

Duke University; Duke University; Duke University; Duke University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The energy consumption of building for heating and cooling accounts for about 15% of the total energy consumption of the world. Owing to the rapid progress in nanophotonic materials, innovative technologies based on multispectral design and tuning have obtained significant development and provided new opportunities to decrease the energy consumption of buildings. Based on this background, this review aims to summarize state-of-the-art progress of daytime radiative cooling, smart windows, and personal thermal management toward net-zero energy buildings based on multispectral material and photonic engineering. Unsolved scientific and technical challenges associated with future perspectives in this field are also discussed, hoping to promote the development of building energy-saving technologies for our sustainable future.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.0c00322

Chinese Library Classification Number:

Citation Information:

The energy consumption of building for heating and cooling accounts for about 15% of the total energy consumption of the world. Owing to the rapid progress in nanophotonic materials, innovative technologies based on multispectral design and tuning have obtained significant development and provided new opportunities to decrease the energy consumption of buildings. Based on this background, this review aims to summarize state-of-the-art progress of daytime radiative cooling, smart windows, and personal thermal management toward net-zero energy buildings based on multispectral material and photonic engineering. Unsolved scientific and technical challenges associated with future perspectives in this field are also discussed, hoping to promote the development of building energy-saving technologies for our sustainable future.

quote

GB/T 7714-2015 [1] Xiuqiang Li, Wanrong Xie, Chenxi Sui, et al. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.0c00322.
MLA [1] Xiuqiang Li, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.0c00322.
APA [1] Xiuqiang Li, Wanrong Xie, Chenxi Sui, & PoChun Hsu. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.0c00322
IEEE [1] Xiuqiang Li, Wanrong Xie, Chenxi Sui, and PoChun Hsu, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.0c00322.