Controlling the Organization of PEDOT:PSS on Cellulose Structures AITranslate
Abstract AITranslate
Composites of biopolymers and conducting polymers are emerging as promising candidates for a green technological future and are actively being explored in various applications, such as in energy storage, bioelectronics, and thermoelectrics. While the device characteristics of these composites have been actively investigated, there is limited knowledge concerning the fundamental intracomponent interactions and the modes of molecular structuring. Here, by use of cellulose and poly(3,4-ethylenedioxythiophene):poly(styrenesulfonate) (PEDOT:PSS), it is shown that the chemical and structural makeup of the surfaces of the composite components are critical factors that determine the materials organization at relevant dimensions. AFM, TEM, and GIWAXS measurements show that when mixed with cellulose nanofibrils, PEDOT:PSS organizes into continuous nanosized beadlike structures with an average diameter of 13 nm on the nanofibrils. In contrast, when PEDOT:PSS is blended with molecular cellulose, a phase-segregated conducting network morphology is reached, with a distinctly relatively lower electric conductivity. These results provide insight into the mechanisms of PEDOT:PSS crystallization and may have significant implications for the design of conducting biopolymer composites for a vast array of applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.9b00444
Chinese Library Classification Number:
Citation Information:
Composites of biopolymers and conducting polymers are emerging as promising candidates for a green technological future and are actively being explored in various applications, such as in energy storage, bioelectronics, and thermoelectrics. While the device characteristics of these composites have been actively investigated, there is limited knowledge concerning the fundamental intracomponent interactions and the modes of molecular structuring. Here, by use of cellulose and poly(3,4-ethylenedioxythiophene):poly(styrenesulfonate) (PEDOT:PSS), it is shown that the chemical and structural makeup of the surfaces of the composite components are critical factors that determine the materials organization at relevant dimensions. AFM, TEM, and GIWAXS measurements show that when mixed with cellulose nanofibrils, PEDOT:PSS organizes into continuous nanosized beadlike structures with an average diameter of 13 nm on the nanofibrils. In contrast, when PEDOT:PSS is blended with molecular cellulose, a phase-segregated conducting network morphology is reached, with a distinctly relatively lower electric conductivity. These results provide insight into the mechanisms of PEDOT:PSS crystallization and may have significant implications for the design of conducting biopolymer composites for a vast array of applications.
quote
| GB/T 7714-2015 | [1] Dagmawi Belaineh, Jens W. Andreasen, Justinas Palisaitis, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00444. |
| MLA | [1] Dagmawi Belaineh, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00444. |
| APA | [1] Dagmawi Belaineh, Jens W. Andreasen, Justinas Palisaitis, Abdellah Malti, Karl Håkansson, Lars Wågberg, Xavier Crispin, Isak Engquist, & Magnus Berggren. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00444 |
| IEEE | [1] Dagmawi Belaineh, Jens W. Andreasen, Justinas Palisaitis, Abdellah Malti, Karl Håkansson, Lars Wågberg, Xavier Crispin, Isak Engquist, and Magnus Berggren, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00444. keywords: {nanocomposites;biomaterials;PEDOT;nanotechnology;energy materials;cellulose} |