Biomimetic and Hydrophilic Vitamin B5 Analogous Methacrylamide Polymers Prevent Surface Fouling AITranslate
Abstract AITranslate
This study reports the synthesis of well-defined polymers of vitamin B5 analogous methacrylamide (poly(B5AMA)) using the reversible addition fragmentation chain transfer polymerization method. The prepared telechelic poly(B5AMA) with a predicted molecular weight and narrow polydispersities are grafted onto silanized glass surfaces using a “grafting to” approach. The polymer-treated samples are characterized for the water contact angle and surface roughness properties, as a function of polymer size and density of the polymers grafted onto the glass slides. The antifouling behavior of poly(B5AMA)-grafted glass slides is then studied and compared with that of PEGylated glass slides, upon treatment with a variety of proteins and bacteria. The functionalized surfaces exhibit remarkable antifouling properties that are found to be dependent on both the density and the molecular weight of the grafted polymers.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c01505
Chinese Library Classification Number:
Citation Information:
This study reports the synthesis of well-defined polymers of vitamin B5 analogous methacrylamide (poly(B5AMA)) using the reversible addition fragmentation chain transfer polymerization method. The prepared telechelic poly(B5AMA) with a predicted molecular weight and narrow polydispersities are grafted onto silanized glass surfaces using a “grafting to” approach. The polymer-treated samples are characterized for the water contact angle and surface roughness properties, as a function of polymer size and density of the polymers grafted onto the glass slides. The antifouling behavior of poly(B5AMA)-grafted glass slides is then studied and compared with that of PEGylated glass slides, upon treatment with a variety of proteins and bacteria. The functionalized surfaces exhibit remarkable antifouling properties that are found to be dependent on both the density and the molecular weight of the grafted polymers.
quote
| GB/T 7714-2015 | [1] Diego Combita, Nauman Nazeer, Adnan Murad Bhayo, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01505. |
| MLA | [1] Diego Combita, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01505. |
| APA | [1] Diego Combita, Nauman Nazeer, Adnan Murad Bhayo, & Marya Ahmed. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01505 |
| IEEE | [1] Diego Combita, Nauman Nazeer, Adnan Murad Bhayo, and Marya Ahmed, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01505. keywords: {RAFT polymerization;hydrophilic polymers;polymer brushes;grafted polymers;antifouling surfaces} |