Fabrication of Shaped Chitin Fibers by Gradient Regeneration Combined with a Physical Pressure Method AITranslate

Wuhan Textile University; Huazhong University of Science & Technology; Wuhan Textile University; Hubei University of Automotive Technology; Wuhan Textile University; Wuhan Textile University; Wuhan Textile University; Wuhan Textile University; Wuhan Textile University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The exigency within the textile industry for molded fibers has become increasingly pronounced, owing to the coveted attributes inherent in planar fiber products, namely, their luxuriant tactile quality, ethereal weightiness, and avant-garde allure. In this investigation, we propose a pioneering methodology for the synthesis of planar chitin fibers, diverging from the conventional paradigm of spinneret design for fiber shaping. Analytical methodologies, encompassing Fourier-transform infrared spectroscopy (FT-IR), X-ray diffraction (XRD), and optical microscopy, were judiciously harnessed to unravel the intricacies of the fiber formation process. By subjecting chitin fibers to coagulation baths infused with phytic acid, a stratified dermal-core architecture was engendered, endowing the fibers with remarkable malleability under exogenic forces, thereby culminating in the homogeneous production of planar chitin fibers. Thorough scrutiny through optical microscopy and cross-sectional analysis substantiates the efficacy of this innovative approach. These revelations not only bestow invaluable insights into the fabrication of planar fibers but also broaden the horizons of potential chitin applications across multifarious domains.

KeyWords AITranslate

chitin alkali/urea shaped fiber skincore structure wet spinning
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c02277

Chinese Library Classification Number:

Citation Information:

The exigency within the textile industry for molded fibers has become increasingly pronounced, owing to the coveted attributes inherent in planar fiber products, namely, their luxuriant tactile quality, ethereal weightiness, and avant-garde allure. In this investigation, we propose a pioneering methodology for the synthesis of planar chitin fibers, diverging from the conventional paradigm of spinneret design for fiber shaping. Analytical methodologies, encompassing Fourier-transform infrared spectroscopy (FT-IR), X-ray diffraction (XRD), and optical microscopy, were judiciously harnessed to unravel the intricacies of the fiber formation process. By subjecting chitin fibers to coagulation baths infused with phytic acid, a stratified dermal-core architecture was engendered, endowing the fibers with remarkable malleability under exogenic forces, thereby culminating in the homogeneous production of planar chitin fibers. Thorough scrutiny through optical microscopy and cross-sectional analysis substantiates the efficacy of this innovative approach. These revelations not only bestow invaluable insights into the fabrication of planar fibers but also broaden the horizons of potential chitin applications across multifarious domains.

quote

GB/T 7714-2015 [1] Yaoting Liang, Ning Jiang, Xinglin Liu, et al. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c02277.
MLA [1] Yaoting Liang, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c02277.
APA [1] Yaoting Liang, Ning Jiang, Xinglin Liu, Ling Nie, Dengpeng Song, Liquan Jiang, Hao Yu, Weilin Xu, & Kunkun Zhu. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c02277
IEEE [1] Yaoting Liang, Ning Jiang, Xinglin Liu, Ling Nie, Dengpeng Song, Liquan Jiang, Hao Yu, Weilin Xu, and Kunkun Zhu, ACS Applied Polymer Materials, no. 6, 2024, doi: 10.1021/acsapm.3c02277. keywords: {chitin;alkali/urea;shaped fiber;skincore structure;wet spinning}